A first-principles study on properties of Ni/Ni3Al interfaces with Re and Ru addition
湖南大学 材料科学与工程学院
Cite this article: 

. A first-principles study on properties of Ni/Ni3Al interfaces with Re and Ru addition. Acta Metall Sin, 2007, 43(2): 137-143 .

Download:  PDF(759KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Energetics and electronic structures of Ni/Ni3Al interface with additions of Re and Ru have been investigated by a first-principles plane-wave pseudopotential method. The calculated rupture works W show both of that either Re substitutes for Ni in g-Ni block or Ru replaces for Al atoms in g¢-Ni3Al block are profitable to improve the strength of the Ni/Ni3Al interface. In the case of the multiple alloying of Re and Ru, it is found only the mode of Re and Ru, respectively, occupying at Ni and Al sites at (001) atomic layers adjacent to the coherent (002) interfacial atomic layer can further enhance the Ni/Ni3Al interface. While Ru locates at Al sites in g¢-Ni3Al block and far away from the coherent (002) interfacial layer, it is found the multiple alloying of Re and Ru not only do not elevate the strengths of Ni/Ni3Al interface with addition of Re or Ru but make them decrease to a lower value than that of clear Ni/Ni3Al interface without addition as well. A deep analysis of electron densities of states (DOS) and the distributions of valence electron densities of Ni/Ni3Al interface before and after alloying reveals that the effect of Re and Ru alloying on the rupture strength of g-Ni/g¢-Ni3Al interface can be attributed to the change of the interlayer bonding in the interfacial region induced by strong electron interactions within first nearest neighbor (FNN) Re-Ni and Ru-Ni atoms, respectively, compared with FNN Ni-Ni and Ni-Al.
Key words:  g-Ni/g¢      alloying effect      first-principle calculation      electron structure      
Received:  10 April 2006     
ZTFLH:  TG132.33  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I2/137

[1]Ofori A P,Rossouw C J,Humphreys C J.Acta Mater,2005;53:97
[2]Wanderka N,Glatzel U.Mater Sci Eng,1995;A203:69
[3]Warren P J,Cerezo A,Smith G D W.Mater Sci Eng,1998;A250:88
[4]Darolia R,Lahrman D F,Field R D.In:Rerchman S,Duhl D N,Maurer G,Antolovich S,Lund C eds.,Superalloys 1988,Warrendale,PA:TMS,1988:255
[5]Harada H.In:Lecomte-Beckers J,Schubert F,Ennis P J eds.,Superalloys:Materials for Advanced Power Engineering 1998,Vol.5Ⅲ.Jülich,German:University de Liege European Commission,1998:131
[6]Liu L M,McAllister B,Ye H Q,Hu P.J Am Chem Soc,2006;128:4017
[7]Liu Y,Chen K Y,Lu G,Zhang J H,Hu Z Q.Acta Mater,1997;45:1837
[8]Chen K,Zhao L R,Tse J S.Mater Sci Eng,2004;A365:8O
[9]Chen K,Zhao L R,Tse J S.Mater Sci Eng,2003;A360:197
[10]Chen K,Zhao L R,Tse J S.Acta Mater,2003;51:1079
[11]Chen K,Zhao L R,Tse J S.Philos Mag,2003;83:1685
[12]Peng P,Jin Z H,Yang R,Hu Z Q.J Mater Sci,2004;39:3957
[13]Peng P,Zhou D W,Liu J S,Yang R,Hu Z Q.Mater Sci Eng,2006;A416:169
[14]Peng P,Soh A K,Yang R,Hu Z Q.Comput Mater Sci,2006;38:354
[15]Segall M D,Lindan Philip J D,Probert M J,Pickard C J,Hasnip PJ,Clark S J,Payne M C.J Phys:Condens Matter,2002;14:2717
[16]Vanderbilt D.Phys Rev,1990;41B:7892
[17]Francis G P,Payne M C.J Phys:Condens Matter,1990;2:4395
[18]Pulay P.Mol Phys,1969;17:197
[19]Fischer T H.J Phys Chem,1992;96:9768
[20]Harada H,Ishida A,Bhadeshia H K D H,Bhadeshia,Yamazaki M.Appl Surf Sci,1993;67:299
[21]Hu Q M,Yang R,Xu D S,Hao Y L,Li D.Phys Rev,2003;67B:224203
[22]Boettger J C.Phys Rev,1994;49B:16798
[23]Caron P,Khan T.Aerospace Sci Technol,1999;3:513
[24]Fu C L,Yoo M H.Mater Chem Phys,1992;32:25
[1] MAO Fei, LU Hao, TANG Fawei, GUO Kai, LIU Dong, SONG Xiaoyan. First-Principle Calculation on the Effect of Mn and In on the Structural Stability and Magnetic Moment of SmCo7 Alloys[J]. 金属学报, 2021, 57(7): 948-958.
[2] Jing BAI,Ze LI,Zhen WAN,Xiang ZHAO. A First-Principles Study on Crystal Structure, Phase Stability and Magnetic Properties of Ni-Mn-Ga-Cu Ferromagnetic Shape Memory Alloys[J]. 金属学报, 2017, 53(1): 83-89.
[3] HUANG Lian, GAO Kunyuan, WEN Shengping, HUANG Hui, WANG Wei, NIE Zuoren. VALENCE ELECTRON STRUCTURE ANALYSIS OF EQUILIBRIUM AND METASTABLE PHASES OF Al3M(M=Ti, Zr, Hf)[J]. 金属学报, 2012, 48(4): 492-501.
[4] ZHAO Yufei FU Yuechun HU Qingmiao YANG Rui. FIRST-PRINCIPLES INVESTIGATIONS OF LATTICE PARAMETERS, BULK MODULI AND PHASE STABILITIES OF Ti1-xVx AND Ti1-xNbx ALLOYS[J]. 金属学报, 2009, 45(9): 1042-1048.
[5] LIU Zhilin; LIU Weidong; LIN Cheng. STRENGTH CALCULATION AND ITS PREDICTION OF NON QUENCHED-TEMPERED STEEL DURING CONTINUOUS CASTING-ROLLING[J]. 金属学报, 2004, 40(12): 1248-1252 .
[6] ZHU Ruifu; LU Yupeng; CHEN Chuanzhong; LI Shitong; WANG Shiqing (Shandong University of Technology; Jinan 250061) ZHANG Fucheng (Yanshan University; Qinhuangdao 066004). AN ANALYSIS OF VALENCE ELECTRON STRUCTURE OF Fe-C-Mn ALLOYING AUSTENITE[J]. 金属学报, 1996, 32(6): 561-564.
[7] ZHANG Jianmin(Central Iron and Steel Research Institute;Ministry;of Metallurgical Industry;Beijing 100081)ZHANG Ruilin;YU Ruihuang(Jilin University;Changchun 130023)(Manuscript received 1994-08-29;in revised form 1995-02-05). HYDROGEN EMBRITTLEMENT BEHAVIOUR IN Fe_3Al[J]. 金属学报, 1995, 31(7): 300-303.
[8] LI Musen; FU Shaoli(Shandong University of Technology; Jinan 250014). XU Wandong(Tianjin University; Mianjin 300072); ZHANG Ruilin. YU Ruihuang(Jilin University; Changchun 130023). VALENCE ELECTRON STRUCTURE OF Fe_2B PHASE AND ITS EIGEN-BRITTLENESS[J]. 金属学报, 1995, 31(5): 201-208.
[9] ZHENG Yasgzeng;ZHANG Fucheng Yanshan University; Qinhuangdao. EFFECT OF HETEROGENEOUS DISTRIBUTION OF C AND ALLOYING ELEMENTS ON γ/α′ TRANSFORMATION IN A Fe-Mn-Cr-C ALLOY[J]. 金属学报, 1991, 27(3): 82-85.
No Suggested Reading articles found!