Abstract The effect of macrostructure and casting temperature on susceptibility to hydrogen flaking、the fracture toughness, KIQ, and threshold stress intensity factor of hydrogen induced delayed cracking, KIH, have been investigated. The result shows that casting temperature can influence the susceptibility to hydrogen flaking, which of the last billet is higher then that of the first billet. There is evident effect of macrostructure on the susceptibility to hydrogen flaking, which is the maximum in thezone of cylindrical grain and the minimum in the zone of equal-axis grain. There are no effect of the macrostructure and casting temperature on hydrogen diffusivity, Da, the fracture toughness, KIQ, and the threshold stress intensity factor of hydrogen-induced delayed cracking, KIH.
[1]Pollard M G.Proc Inst Eng,1999;213F:181 [2]Mclellan R R,Xu Z R.Scr Mater,1997;36:1201 [3]Chu W Y.Hydrogen Damage and Hydrogen-Induced Delayed Fracture.Beijing:Metallurgical Industry Press,1988:146(褚武扬.氢损伤与滞后断裂.北京:冶金工业出版社,1988:148) [4]Interrante C G.Current Solution to Problems in Steels.Metals Park,OH:ASM,1982:2 [5]Pressourye G M.Current Solution to Problems in Steels.Metals Park,OH:ASM,1982:18 [6]Steiner J E.Current Solution to Problems in Steels.Metals Park,OH:ASM,1982:55 [7]Oriani R A,Hirth J P,Smialowski M.Hydrogen Degradation of Ferrous Alloys,Park Ridge,N J:Noyes Pub,1985:218 [8]Fruehan R T.Iron Steel Maker,1997;24:61 [9]Ren X C,Chu WY,Li J X,Qiao L J,Jiang B,Chen G,Cui Y H.Acta Metall Sin,2006;42:273(任学冲,褚武扬,李金许,乔利杰,江波,陈刚,崔银会.金属学报,2006;42:273) [10]Ren X C,Shan G G,Chu WY,Su Y J,Gao K W,Qiao L J,Jiang B,Chen G,Cui Y H.Chin Sci Bull,2005;50:1962 [11]Peng X,Su Y J,Gao K W,Qiao L J,Chu W Y.Mater Lett,2004;58:2073 [12]Ren X C,Chu W Y,Li J X,Qiao L J,Jiang B,Chcn G,Cui Y H.Acta Metall Sin,2006;42:153(任学冲,褚武扬,李金许,乔利杰,江波,陈刚,崔银会.金属学报,2006;42:153) [13]Hodge J M,Orehoski M A,Steiner J E.Trans Metall Soc AIME,1964;230:1182 [14]Allen A O.Probability,Statistics and Queuing Theory,New York:Academic Press,1978:293 [15]Wu M,Chu W Y,Li J X,Jiang B,Chen G,Cui Y H.Acta Metall Sin.2006:42:815(武明,褚武扬,李金许,江波,陈刚,崔银会.金属学报,2006;42:815)