| The Effect of Solute Concentration by Solution Treatment on Portevin-Le Chatelier effect in Al-Cu Alloys |
|
Cite this article:
. The Effect of Solute Concentration by Solution Treatment on Portevin-Le Chatelier effect in Al-Cu Alloys. Acta Metall Sin, 2006, 42(12): 1248-1252 .
|
|
|
Abstract In this paper the solute concentration in solid solution and precipitated phase content in alloy are altered by solution treatment at different temperature. The influence on dislocation movement is analyzed by test result, and the micro-mechanism of dynamic strain aging (DSA) is discussed. In the test, when solution treatment temperature reduces stepwise from 500℃, the amplitude of the serrated flow decreases until it reaches minimum at 300℃. And the amplitude increases on the contrary when solution treatment temperature reducing unceasingly to 100℃. When solution treatment temperature is higher than 300℃, solute concentration is the key factor of DSA and its increasing leads to the enhancing of DSA. When solution treatment temperature is lower than 300℃, the intensity of DSA is determined by precipitated phase density and enhances with it increasing.
|
|
Received: 08 March 2006
|
|
|
[1] Bell J F. Encyclopedia of Physics, Mechanics of Solids I. Berlin: Springer-Verlag Press, 1973: 41, 649 [2] Munz D, Macherauch E. Z Metallkd, 1966; 57: 552 [3] Mulford R A, Kocks U F. Acta Metall, 1979; 27: 1125 [4] Tian B H, Li H X, Zhang Y G, Chen C Q. Acta Metall Sin, 1998; 34: 603 (田宝辉,李焕喜,张永刚,陈昌麒.金属学报.1998;34:603) [5] Jiang H F, Zhang Q C, Jiang Z Y, Wu X P. Acta Metall Sin, 2005; 41: 727 (江慧丰,张青川,蒋震宇,伍小平.金属学报,2005;41:727) [6] Chihab K, Estrin Y, Kubin L P. Scr Metall, 1987; 21: 203 [7] Jiang H F, Zhang Q C, Jiang Z Y, Chen Z J, Wu X P. Chin Phys Lett, 2005; 22: 99 (江慧丰,张青川,蒋震宇,陈忠家.伍小平.中国物理快报, 2005;22:99) [8] Pink E, Grinberg A. Mater Sci Eng, 1981; A51: 1 [9] McCormick P G. Trans Indian Inst Met, 1986; 39: 98 [10] Chihab K, Estrin Y, Kubin LP, Vergnol J. Scr Metall, 1987; 21: 203 [11] Jiang Z Y, Zhang Q C, Jiang H F, Chen Z J, Wu X P. Mater Sci Eng, 2005; A403: 154 [12] Cottrell A H. Dislocations and Plastic Flow in Crystals. London: Oxford University Press, 1953: 1 [13] Wang C, Xu Y B, Han E H. Acta Metall Sin, 2006; 42: 191 (王聪,徐永波,韩恩厚.金属学报, 2006;42:191) [14] McCormick P G. Acta Metall, 1972; 20: 351 [15] Estrin Y, Kubin L P. In: Muhlhaus H B, ed., Continum Models for Materials With Microstructures, New York: John Wiley & Sons Ltd., 1995: 395 [16] Rizzi E, Hahner P. Int J Plast, 2004; 20: 121 [17] Picu R C. Acta Mater, 2004; 52: 3447 [18] Picu R C, Vincze G, Ozturk F, Gracio J J, Barlat F, Ma- niatty A M. Mater Sci Eng, 2005; A390: 334 [19] Chen Z J, Zhang Q C, Jiang Z Y, Jiang H F, Wu X P. J Mater Sci Technol, 2004; 20: 535 [20] Jiang H F, Zhang Q C, Xu Y H, Wu X P. Acta Metall Sin, 2006; 42: 139 (江慧丰,张青川,徐毅豪,伍小平.金属学报,2006;42:139) [21] Jiang H F, Zhang Q C, Xu Y H, Wu X P. Acta Phys Sin, 2006; 55: 409 (江慧丰,张青川,徐毅豪,伍小平.物理学报,2006;55:409) [22] Lu J Y, Jiang Z Y, Zhang Q C. Acta Metall Sin, 2006; 42: 6 (卢俊勇,蒋震宇,张青川.金属学报, 2006;42:6) [23] Zhang S L, Ren S Z. Concise Manual of Aluminum Alloy. Shanghai: Shanghai Scientific and Technological Literature Press, 2001: 11 (张士林,任颂赞.简明铝合金手册.上海:上海科学技术文献出版社,2001:11) [24] Zhang Q C, Jiang Z Y, Jiang H F, Chen Z J, Wu X P. Int J Plast, 2005; 21: 2150 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|