| GIANT MAGNETO-IMPEDANCE EFFECTS OF AS DEPOSITED FeZrBNi SANDWICHED FILMS |
| YUAN Huimin; JIANG Shan; WANG Wenjing; YAN Shishen;XIAO Shuqin |
| 山东大学物理与微电子学院; 济南 250100 |
|
Cite this article:
YUAN Huimin; JIANG Shan; WANG Wenjing; YAN Shishen; XIAO Shuqin. GIANT MAGNETO-IMPEDANCE EFFECTS OF AS DEPOSITED FeZrBNi SANDWICHED FILMS. Acta Metall Sin, 2006, 42(9): 971-973 .
|
|
|
Abstract Giant magneto-impedance (GMI) effects of FeZrBNi/Ag/FeZrBNi sandwiched films prepared by radio frequency sputtering on the substrate of single crystal Si have been measured. The maximum GMI ratios are 18% and 31% in longitudinal and transverse fields at 7 MHz and 8 MHz, respectively. Corresponding, the maximum effective susceptibility ratios are 153% (at 7 MHz) and 5117% (at 8 MHz) for longitudinal and transverse cases, respectively, indicating that the as-deposited FeZrBNi/Ag/FeZrBNi films have good sof magnetic properties and GMI effect.
|
|
Received: 28 February 2006
|
|
|
[1]Mohri K,Kohzawa T,Kawashima K,Yoshida H,Panina L V.IEEE Trans Magn,1992;28:3150 [2]Suzuki K,Makino A,Inoue A,Masumoto T.J Appl Phys,1993;74:3316 [3]Kojima A,Makino A,Kawamura Y,Inoue A,Masumoto T.J Appl Phys,1996;35:L19 [4]Suzuki K,Makino A,Inoue A,Masumoto T.J Appl Phys,1991;70:6232 [5]Ye C Q,Yan B,Xu Z.Shanghai Nonferrous Met,2005;26:36(叶超群,严彪,徐政.上海有色金属,2005;26:36) [6]Li X D,Yuan W Z,Zhao Z J,Ruan J Z,Yang X L.Funct Mater,2004;35:686(李晓东,袁望治,赵振杰,阮建中,杨燮龙.功能材料,2004;35:686) [7]Hika K,Panina L V,Mohri K.IEEE Traus Magn,1996;32:4594 [8]Dai Y Y,Liu Y H,Xiao S Q,Zhang L,Wu H Z,Zhang Y Z.Acta Metall Sin,2001;37:277(代由勇,刘宜华,萧淑琴,张林,吴厚政,张延忠.金属学报,2001;37:277) [9]Chen W P,Xiao S Q,Wang W J,Liu Y H.Acta Metall Sin,2004;40:1295(陈卫平,萧淑琴,王文静,刘宜华.金属学报,2004;40:1295) [10]Yu J Q,Zhou Y,Cai B C,Zhao X L.Funct Mater,2001;32:136(禹金强,周勇,蔡炳初,赵小林.功能材料,2001;32:136)d |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|