Effect of Casting Temperature on Mechanical Properties of SiC Foam/SiCp/Al Hybrid Composites
ZHAO Longzhi; CAO Xiaoming; TIAN Chong; HU Wanping; XING Hongwei; ZHANG Jinsong
Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016
Cite this article: 

ZHAO Longzhi; CAO Xiaoming; TIAN Chong; HU Wanping; XING Hongwei; ZHANG Jinsong. Effect of Casting Temperature on Mechanical Properties of SiC Foam/SiCp/Al Hybrid Composites. Acta Metall Sin, 2006, 42(1): 103-108 .

Download:  PDF(1519KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  01 June 2005     
ZTFLH:  TB333  
  TG113.25  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I1/103

[1]Ibrahim I A.J Mater Sci,1991;26:1137
[2]Lloyd D J.Int Mater Rev,1994;39(1):1
[3]Clarke D R.J Am Ceram Soc,1992;75:739
[4]Peng H X,Fan Z,Evans J R G.Mater Eng,2001;A303:37
[5]Tanihata K,Suganuma K.Key Eng Mater,1999;161-163:259
[6]Bakis C E,Nannl A,Turosky J A,Koehler S W.Comp Sci Technol,2001;61:815
[7]Roerden A M,Herakovich C I.Composite Sci Technol,2001;60:2443
[8]Zhou C H,Liu W,Li X M,Jiang B.Fiber Reinf Plast/Composite,2000;(2):32(周春华,刘威,李学闵,姜波.玻璃钢/复合材料,2000;(2):32)
[9]Haga O,Koyama H,Kawada K.Adv Comp Mater,1996;5(2):225
[10]Fang X D,Yang H C,AN Z R.Aerosp Mater Technol,2002;32:38(方旭东,杨鸿昌,安章荣.宇航材料工艺,2002;32:38)
[11]Chadwick G A,Yue T M.Met Mater,1989;5(1):6
[12]Hemambar C,Rao B S,Jayaram V.Mater Manuf Process,2001;16:779
[13]Pech-Canul M I,Makhlouf M M.J Mater Synth Process,2000;8(1):35
[14]Yang L J.J Mater Prog Technol,2003;140:391
[15]Zhao L Z,Cao X M,Tian C,Hu W P,Xing H W,Zhang J S.Chin J Mater Res,2005;19:512(赵龙志,曹小明,田冲,胡宛平,邢宏伟,张劲松.材料研究学报,2005;19:512)
[16]Zhao L Z,Cao X M,Tian C,Hu W P,Xing H W,Zhang J S.Chin J Mater Res,2005;19:485(赵龙志,曹小明,田冲,胡宛平,邢宏伟,张劲松.材料研究学报,2005;19:485)
[17]Rohatigi P K,Pasciak K,Narendranath C S.J Mater Sci,1994;9:5357
[18]Zhang Z H,Bian X F,Qin J Y,Wang W M,Liu X F.Acta Metall Sin,2000;36:33(张忠华,边秀房,秦敬玉,王伟民,刘相法.金属学报,2000;36:33)
[19]Sun M H,Geng H R,Bian X F,Liu Y.Acta Metall Sin,2000;36:1134(孙民华,耿浩然,边秀房,刘燕.金属学报,2000;36:1134)
[20]Li X Z,Bian X F.Chin J Foundry,2000;49:1(李喜珍,边秀房.铸造,2000;49:1)j
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!