Corrosion Resistance of NiTiNb Shape Memory Alloy as Pipe Coupling
TAO Binwu; LI Songmei; LIU Jianhua; LI Jiafeng; SHI Junxiu
School of Materials Science and Engineering; Beijing University of Aeronautics and Astronautics; Beijing 100083
Cite this article: 

TAO Binwu; LI Songmei; LIU Jianhua; LI Jiafeng; SHI Junxiu. Corrosion Resistance of NiTiNb Shape Memory Alloy as Pipe Coupling. Acta Metall Sin, 2006, 42(1): 99-102 .

Download:  PDF(838KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  18 April 2005     
ZTFLH:  TG174  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I1/99

[1]Duerig T W.Mater Sci Form,1990;56-58:679
[2]Piao M,Miyazakai S,Otsuka K.Mater Trans JIM,1992;33:337
[3]Cai W,Zhang C C.J Mater Sci Technol,1994;10:27
[4]Yang H B,Ying W H,Lin J Y,Zhang X M,Guo J H.Rare Metal Mater Eng,1999;28:81(杨华斌,殷为宏,吝靖玉,张小明,郭继红.稀有金属材料与工程,1999:28:81)
[5]Mo H Q,Li C,Wang C H,Qiu S Y,Huang D C.Nuclear Power Eng,2003;24:559(莫华强,李聪,王丛林,邱绍宇,黄德成,沈保罗.核动力工程,2003:24:559)
[6]He X M,Rong L J,Yan D S,Jiang Z M,Li Y Y.Acta Metall Sin,2004;40:721(何向明,戎利建,阎德胜,姜志民,李依依.金属学报,2004;40:721)
[7]Tao B W,Liu J H,Li S M.Acta Metall Sin,2005;41:337(陶斌武,刘建华,李松梅.金属学报,2005:41:337)
[8]Dong Z Z,Liu W X,Jia D,Tang Z L,Wang D F.Rare Metal Mater Eng,2000;29:182(董治中,刘文西,贾堤,唐子龙,王德法.稀有金属材料与工程,2000;29:182)
[9]Xu C H,Ma X Q,Shi S Q,Wo C H.Mater Sci Eng,2004;A371:45
[10]Cao C N.The Principle of Corrosion Electrochemistry.Beijing:Chemical Industry Press,1985:210(曹楚南.腐蚀电化学原理.北京:化学工业出版社,1985;210)
[11]Rondelli G,Vicentini B,Cigada A.Corros Sci,1990;30:8O5
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!