| Effect of Casting Temperature on Mechanical Properties of SiC Foam/SiCp/Al Hybrid Composites |
| ZHAO Longzhi; CAO Xiaoming; TIAN Chong; HU Wanping; XING Hongwei; ZHANG Jinsong |
| Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
ZHAO Longzhi; CAO Xiaoming; TIAN Chong; HU Wanping; XING Hongwei; ZHANG Jinsong. Effect of Casting Temperature on Mechanical Properties of SiC Foam/SiCp/Al Hybrid Composites. Acta Metall Sin, 2006, 42(1): 103-108 .
[1]Ibrahim I A.J Mater Sci,1991;26:1137 [2]Lloyd D J.Int Mater Rev,1994;39(1):1 [3]Clarke D R.J Am Ceram Soc,1992;75:739 [4]Peng H X,Fan Z,Evans J R G.Mater Eng,2001;A303:37 [5]Tanihata K,Suganuma K.Key Eng Mater,1999;161-163:259 [6]Bakis C E,Nannl A,Turosky J A,Koehler S W.Comp Sci Technol,2001;61:815 [7]Roerden A M,Herakovich C I.Composite Sci Technol,2001;60:2443 [8]Zhou C H,Liu W,Li X M,Jiang B.Fiber Reinf Plast/Composite,2000;(2):32(周春华,刘威,李学闵,姜波.玻璃钢/复合材料,2000;(2):32) [9]Haga O,Koyama H,Kawada K.Adv Comp Mater,1996;5(2):225 [10]Fang X D,Yang H C,AN Z R.Aerosp Mater Technol,2002;32:38(方旭东,杨鸿昌,安章荣.宇航材料工艺,2002;32:38) [11]Chadwick G A,Yue T M.Met Mater,1989;5(1):6 [12]Hemambar C,Rao B S,Jayaram V.Mater Manuf Process,2001;16:779 [13]Pech-Canul M I,Makhlouf M M.J Mater Synth Process,2000;8(1):35 [14]Yang L J.J Mater Prog Technol,2003;140:391 [15]Zhao L Z,Cao X M,Tian C,Hu W P,Xing H W,Zhang J S.Chin J Mater Res,2005;19:512(赵龙志,曹小明,田冲,胡宛平,邢宏伟,张劲松.材料研究学报,2005;19:512) [16]Zhao L Z,Cao X M,Tian C,Hu W P,Xing H W,Zhang J S.Chin J Mater Res,2005;19:485(赵龙志,曹小明,田冲,胡宛平,邢宏伟,张劲松.材料研究学报,2005;19:485) [17]Rohatigi P K,Pasciak K,Narendranath C S.J Mater Sci,1994;9:5357 [18]Zhang Z H,Bian X F,Qin J Y,Wang W M,Liu X F.Acta Metall Sin,2000;36:33(张忠华,边秀房,秦敬玉,王伟民,刘相法.金属学报,2000;36:33) [19]Sun M H,Geng H R,Bian X F,Liu Y.Acta Metall Sin,2000;36:1134(孙民华,耿浩然,边秀房,刘燕.金属学报,2000;36:1134) [20]Li X Z,Bian X F.Chin J Foundry,2000;49:1(李喜珍,边秀房.铸造,2000;49:1)j |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|