| Corrosion Resistance of NiTiNb Shape Memory Alloy as Pipe Coupling |
| TAO Binwu; LI Songmei; LIU Jianhua; LI Jiafeng; SHI Junxiu |
| School of Materials Science and Engineering; Beijing University of Aeronautics and Astronautics; Beijing 100083 |
|
Cite this article:
TAO Binwu; LI Songmei; LIU Jianhua; LI Jiafeng; SHI Junxiu. Corrosion Resistance of NiTiNb Shape Memory Alloy as Pipe Coupling. Acta Metall Sin, 2006, 42(1): 99-102 .
[1]Duerig T W.Mater Sci Form,1990;56-58:679 [2]Piao M,Miyazakai S,Otsuka K.Mater Trans JIM,1992;33:337 [3]Cai W,Zhang C C.J Mater Sci Technol,1994;10:27 [4]Yang H B,Ying W H,Lin J Y,Zhang X M,Guo J H.Rare Metal Mater Eng,1999;28:81(杨华斌,殷为宏,吝靖玉,张小明,郭继红.稀有金属材料与工程,1999:28:81) [5]Mo H Q,Li C,Wang C H,Qiu S Y,Huang D C.Nuclear Power Eng,2003;24:559(莫华强,李聪,王丛林,邱绍宇,黄德成,沈保罗.核动力工程,2003:24:559) [6]He X M,Rong L J,Yan D S,Jiang Z M,Li Y Y.Acta Metall Sin,2004;40:721(何向明,戎利建,阎德胜,姜志民,李依依.金属学报,2004;40:721) [7]Tao B W,Liu J H,Li S M.Acta Metall Sin,2005;41:337(陶斌武,刘建华,李松梅.金属学报,2005:41:337) [8]Dong Z Z,Liu W X,Jia D,Tang Z L,Wang D F.Rare Metal Mater Eng,2000;29:182(董治中,刘文西,贾堤,唐子龙,王德法.稀有金属材料与工程,2000;29:182) [9]Xu C H,Ma X Q,Shi S Q,Wo C H.Mater Sci Eng,2004;A371:45 [10]Cao C N.The Principle of Corrosion Electrochemistry.Beijing:Chemical Industry Press,1985:210(曹楚南.腐蚀电化学原理.北京:化学工业出版社,1985;210) [11]Rondelli G,Vicentini B,Cigada A.Corros Sci,1990;30:8O5 |
| No Suggested Reading articles found! |
|
|