Stress-Induced Martensite Transformation and Its Reversibility in Cu-18.4Al-8.7Mn-3.4Zn-0.1Zr Alloy
LI Zhou; WANG Mingpu; XU Genying; CHENG Jianyi; ZHANG Bingli
Department of Materials Science and Engineering; Central South University; Changsha 410086; School of Materials Science and Engineering; Hefei University of Technology; Hefei 230009
Cite this article: 

LI Zhou; WANG Mingpu; XU Genying; CHENG Jianyi; ZHANG Bingli. Stress-Induced Martensite Transformation and Its Reversibility in Cu-18.4Al-8.7Mn-3.4Zn-0.1Zr Alloy. Acta Metall Sin, 2003, 39(1): 61-65 .

Download:  PDF(240KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  05 April 2002     
ZTFLH:  TG111.5  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2003/V39/I1/61

[1] Otsuka K. SMM'94, Beijing, 1994; 129
[2] Piao M, Otsuka K, Miyazaki S, Horikawa H. Mater TransJIM, 1993; 34: 919
[3] Zhao L C, Duerig T W, Wayman C M. Scr Metall, 1990;24: 1807
[4] Zhao L H, Cai W. Ada Metall Sin, 1997; 1: 90(赵连城,蔡伟,金属学报,1997;1:90)
[5] Liu W X. SMM'94, Beijing, 1994; 493
[6] Maki T. C-J SMA '97, Hangzhou, 1997; 123
[7] Xu G Y, Wang M P. Trans Met Heat Treat, 1996; 1: 5(徐根应,汪明朴.金属热处理学报, 1996;1:5)
[8] Wang M P, Jin Z P, Yin Z M, Xu G Y. NFsoc, 1995; 4:108
[9] Otansuka K, Wayman C M, Nakai K, Sakamoto H,Shimizu K. Ada Metall, 1976; 24: 207
[10] Horikawa H, Ichinose S, Morii K, Miyazaki S, Otasuka K.Metall Trans A, 1988; 19A: 915
[11] Dai N F, Wei L, Hwang K C. Metall Mater Trans A, 1999;30A: 1933
[12] Kuwano N, Waymen C M. Metal Trans A, 1984; 15A: 621h
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!