Improvement of High-Temperature Oxidation Resistance of TiAl-Based Alloy by Siliconizing Treatment
XIONG Huaping; LI Xiaohong; MAO Wei; LI Jianping; MA Wenli; CHENG Yaoyong
Beijing Institute of Aeronautical Materials; Beijing 100095
Cite this article: 

XIONG Huaping; LI Xiaohong; MAO Wei; LI Jianping; MA Wenli; CHENG Yaoyong. Improvement of High-Temperature Oxidation Resistance of TiAl-Based Alloy by Siliconizing Treatment. Acta Metall Sin, 2003, 39(1): 66-70 .

Download:  PDF(240KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  04 February 2002     
ZTFLH:  TG146.2  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2003/V39/I1/66

[1] Tang Z L, Wang F H, Wu W T. Chin J Mater Res, 1997; 11: 507(唐兆麟,王福会,吴维(?).材料研究学报, 1997;11:507)
[2] Xu D, Zhu H, Tang L J, Yang Y J, Zheng Z H, Liu X H, Taniguchi S, Shibata T. Acta Metall Sin, 1995; 31: B164(徐东,朱宏,汤丽娟,杨云洁,郑志宏,柳襄怀,谷口 滋次,柴田 俊夫.金属学报,1995;31:B164)
[3] Tang Z L, Wang F H, Wu W T. Trans Nonferrous Met, 1998; 8(1) : 56 (唐兆麟,王福会,吴维(?).中国有色金属学报, 1998;8(1) :56)
[4] Wang F H, Tang Z L. Chin J Mater Res, 1998; 12: 337(王福会,唐兆麟.材料研究学报, 1998;12:337)
[5] Peng X, Tang Z L, Li T F, Wu W T. Acta Metall Sin, 1998; 34: 319(彭 晓,唐兆麟,李铁藩,吴维(?).金属学报, 1998;34:319)
[6] He X L, Wang H M, Zheng Q G, Xu D S. Acta Metall Sin, 1998; 34: 983(何秀丽,王华明,郑启光,许德胜.金属学报,1998;34:983)
[7] Kim J P, Jung H G, Kim K Y. Surf Coat Technol, 1999;112: 91
[8] Taniguchi S, Uesaki K. Mater Sci Eng, 1999; A266: 267
[9] He Y H, Huang B Y, Qu X H, Liu Y X. Chin J MaterRes, 1996; 10: 603(贺跃辉,黄伯云,曲选辉,刘业翔.材料研究学报,1996;10:603)
[10] Kim B G, Kim G M, Kim C J. Scr Metall Mater, 1995; 33: 1117
[11] Maki K, Shioda M, Sayashi M. Mater Sci Eng, 1992; A153: 591
[12] Miedema A R, Boer F R, Boom R, Dorleijn J W F. CAL-PHAD, 1977; 1: 353
[13] Kobayashi E, Yoshibara M, Tanaaka R. High Temp Technol, 1990; 8: 179
[14] Taniguchi S, Shibata T, Sakon S. Mater Sci Eng, 1995; A198: 857
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!