| Effect of withdrawal velocity on dendritic interfacial characteristic for Al-Cu alloy during directional solidification |
| Min Qu;Lin LIU;;; |
| 西北工业大学凝固技术国家重点实验室 |
|
Cite this article:
Min Qu; Lin LIU. Effect of withdrawal velocity on dendritic interfacial characteristic for Al-Cu alloy during directional solidification. Acta Metall Sin, 2008, 44(9): 1051-1056 .
|
|
|
Abstract Directional solidification experiments were carried out on Al-4wt%Cu alloy under different withdrawal velocities. It is showed that the primary dendrite arm spacing decreases with increasing withdrawal velocity which is rapid. The solid/liquid interface of dendrite is planar-convex-planar-convex, and it is reinforced first and then weakened and finally almost faded. Dendrite tip temperature is also first increased and then decreased with increasing withdrawal velocity. The KGT model and non-equilibrium effect were used to research the dendrite tip temperature, tip undercooling and composition. This explains the change of dendrite interface morphology well.
|
|
Received: 14 January 2008
|
|
|
[1]Hunt J D.Solidification and Casting of Metals.London: The Metal Society,1979:3 [2]Kurz W,Fisher D J.Acta Metall,1981;29 :11 [3]Trivedi R.Me,all Trans,1984;15A:977 [4]Hunt J D,Lu S Z.Me,all Mater Trans,1996;27A:611 [5]Hunt J D,Lu S Z.Mater Sci Eng,1993;A173:79 [6]Giindiiz M,Cadirh E.Mater Sci Eng,2002;A327:167 [7]Spencer B J,Huppert H E.J Cryst Growth,1999;200: 287 [8](?)stün E,Cadirh E,Kaya H.J Phys:Condens Matter, 2006;18:7825 [9]Kurz W.Adv Eng Mater,2001;3:443 [10]Kurz W,Giovanola B,Trivedi R.Acta Metall,1986;34: 823 [11]Trivrdi R,Kurz W.Acta Metall Mater,1994;42:15 [12]Trivedi R,Kurz W.Int Mater Rev,1994;9(2):49 [13]Bottinger W J,Coriell S R,Trivedi R.In:Mehrabian R, Parrish P A,eds.,Proc 4th Conf on Rapid Solidification Processing:Principles and Technologies,Baton Rouge, LA:Claitor's,Publishing Dir(?)sion,1988:13 [14]Aziz M J.Metall Mater Trans,1996;27A:671 [15]Burden M H,Hunt J D.J Cryst Growth,1974;22:109 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|