| Effect of Cr Content on the Sorption Performance of TiMn1.2-xCrxV0.25Fe0.05 Alloys |
| YU Xuebin; CHEN Jinzhou; WU Zhu; XIA Baojia |
| Shanghai Institute of Microsystem and Information Technology; The Chinese Academy of Sciences; Shanghai 200050 |
|
Cite this article:
YU Xuebin; CHEN Jinzhou; WU Zhu; XIA Baojia. Effect of Cr Content on the Sorption Performance of TiMn1.2-xCrxV0.25Fe0.05 Alloys. Acta Metall Sin, 2004, 40(5): 527-530 .
|
|
|
Abstract The hydrogen absorption-desorption characteristics of
TiMn1.2-xCrxV0.25Fe0.05(x=0.0, 0.1, 0.2, 0.3, 0.4) alloys as a hydrogen storage
tank were investigated. XRD results show that
the lattice constants and the unit cell volume
increase with increasing Cr content. The PCT
results exhibit that the hydrogen sorption plateau
pressure and hysteresis decrease with
increasing Cr content. The change in
the full width half maximum (FWHM) and c/a ratio with
the change in the degree of slope present the same trend
with Cr concentration, which implies that the slope behaviors in
TiMn1.2-xCrxV0.25Fe0.05
system are closely correlated with the
strain energy of interstitial site. In all
cases, the TiMn1.0Cr0.2V0.25Fe0.05 alloy exhibits a larger
hydrogen capacity, lower plateau pressure, and smaller hysteresis and slope properties, which
can satisfy the demand of hydrogen storage tanks for proton exchange
membrane fuel cell.
|
|
Received: 08 May 2003
|
|
|
[1] Mani N, Sivakumar R, Ramaprabhu S. J Alloys Compd, 2002; 337:148 [2] Kim Jin-Ho, Lee Ho, Lee Paul S. J Alloys Compd, 2003; 348:293 [3] Tanaka K, Sowa M, Kita Y, Kubota T, Tanaka N. J Alloys Cornpd, 2002; 330-332:732 [4] Lee Sang-Min, Yu Ji Sang, Lee Ho, Jang Kulk-Jin, Lee Jai-Young. J Alloys Compd, 1999; 293-295:601 [5] Mitrokhin S V, Bezugtaya T N, Verbetaky V N. J Alloys Compd, 2002; 330-332:146 [6] Park Jeong-Gun, Jang Hwan-Young, Han Sang-Cheol, Lee Paul S, Lee Jai-Young. J Alloys Compd, 2001; 325: 293-298 [7] Hong C M, Hao D G, Lin Q Z. d Less-Common Met, 1991; 172-174:1044 [8] Mitrokhin S V, Verbetsky V N. J Alloys Cornpd, 1997; 253-254:201 [9] Hagstrom M T, Klyamkin S N, Lund P D. J Alloys Compd, 1999; 293-295:67 [10] Guther V, Otto A. J Alloys Cornpd, 1999; 293-295:889 [11] Yu X B, Wu Z, Huang T Z. Trans Nonferrous Met Soc Chin, 2003; 13:1116(徐学斌,吴铸,黄太仲.中国有色金属学报,2003;13:1116) [12] Lundin C E, Lynch F E, Magee C B. J Less-Common Met, 1977; 56:19 [13] Ivey D G, Northwood D O. J Mater Sci, 1981; 18:321 [14] Park Jong-Man, Lee Jai-Young. J Less-Common Met, 1991; 167:245 [15] Magee C B, Lju J, Lundin C E. J Less-Common Met, 1981; 78:119 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|