| Microstructure and Properties of A Carbide--Free Bainite-Martensite Ultra--High Strength Steel |
| YANG Fubao; BAI Bingzhe; LIU Dongyu; CHANG Kaidi; WEI Dongyuan; |
| Department of Materials Science and Engineering; Tsinghua University |
|
Cite this article:
YANG Fubao; BAI Bingzhe; LIU Dongyu; CHANG Kaidi; WEI Dongyuan. Microstructure and Properties of A Carbide--Free Bainite-Martensite Ultra--High Strength Steel. Acta Metall Sin, 2004, 40(3): 296-300 .
|
|
|
Abstract The main ideas of component and structure designing for novel high strength and toughness Mn--Si--Cr bainitic steel are presented.Microstructure, delayed fracture mechanism and fatigue property have been analysis based on the excellent mechanical properties. The improvement in
strength and toughness can be contributed to distinctive microstructure of duplex steel. The bainitic carbide is replaced by retained austenite film, which exhibits a better mechanical stability,
thermal stability and chemical stability. The film also acts as a hydrogen trap, inhibiting crack propagation, and lower the susceptibility to hydrogen embrittlement.
|
|
Received: 08 March 2003
|
|
|
[1] Wan D R, Xu C G. High Strength and Ultra-high Strength Steel. Beiiing: China Machine Press. 1988:98(万如,许昌淦.高强度及超高强度钢.北京:机械工业出版社,1988:98) [2] Tomita Y, Okabayashi K. Metall Trans, 1983; 14A:485 [3] Tomita Y, Okawa T. Mater Sci Technol, 1995; 11:245 [4] Tomita Y. Mater Sci Technol, 1995; 11:259 [5] Huang J F, Fang H S, Xu P G, Zheng Y K. Heat Treat Met, 2001; 25(6) : 1(黄进峰,方鸿生,徐平光,郑燕康.金属热处理,2001;25(6) :1) [6] Chen Y T, Fang H S, Bai B Z, Yan Z G, Li Q, Hou C Q, Gao F. Heat Treat Met, 2001; 26(8) : 5(陈颜堂,方鸿生,白秉哲,杨志剐,李琪,侯传基,高凡.金属热处理,2001;26(8) :5) [7] Chu W Y. Hydrogen Induced Failure and Delayed Failure. Beijing: Metallurgy Industry Press, 1988:214(褚武扬.氢损伤和滞后断裂.北京:冶金工业出版社,1988:214) [8] Fuchs H O. Stephens R I. Metal Fatigue in Engineering. New York: John Wiley & Sons. 1980:56 [9] ANSI. MIL-HDBK-5C (Military Material Handbook of America) Change Notice 2. Washington DC: ASTM. 1979 [10] Ritchie R O, Castrocedeno M H, Zackay V F, Parker E R. Met Trans A Phy Met Mater Sci, 1978; 9(1) : 35 [11] Berns H, Wener L. Theor Appl Frac Mech, 1986; (6) : 11 [12] Miihkinen V T T, Edmonds D V. Mater Sci Technol, 1987; 6:441 |