Please wait a minute...
Acta Metall Sin  2004, Vol. 40 Issue (3): 296-300     DOI:
Research Articles Current Issue | Archive | Adv Search |
Microstructure and Properties of A Carbide--Free Bainite-Martensite Ultra--High Strength Steel
YANG Fubao; BAI Bingzhe; LIU Dongyu; CHANG Kaidi; WEI Dongyuan;
Department of Materials Science and Engineering; Tsinghua University
Cite this article: 

YANG Fubao; BAI Bingzhe; LIU Dongyu; CHANG Kaidi; WEI Dongyuan. Microstructure and Properties of A Carbide--Free Bainite-Martensite Ultra--High Strength Steel. Acta Metall Sin, 2004, 40(3): 296-300 .

Download:  PDF(19397KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The main ideas of component and structure designing for novel high strength and toughness Mn--Si--Cr bainitic steel are presented.Microstructure, delayed fracture mechanism and fatigue property have been analysis based on the excellent mechanical properties. The improvement in strength and toughness can be contributed to distinctive microstructure of duplex steel. The bainitic carbide is replaced by retained austenite film, which exhibits a better mechanical stability, thermal stability and chemical stability. The film also acts as a hydrogen trap, inhibiting crack propagation, and lower the susceptibility to hydrogen embrittlement.
Key words:  carbide free bainite      duplex steel      retained austenite           
Received:  08 March 2003     
ZTFLH:  TG142.2  
  TG111  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2004/V40/I3/296

[1] Wan D R, Xu C G. High Strength and Ultra-high Strength Steel. Beiiing: China Machine Press. 1988:98(万如,许昌淦.高强度及超高强度钢.北京:机械工业出版社,1988:98)
[2] Tomita Y, Okabayashi K. Metall Trans, 1983; 14A:485
[3] Tomita Y, Okawa T. Mater Sci Technol, 1995; 11:245
[4] Tomita Y. Mater Sci Technol, 1995; 11:259
[5] Huang J F, Fang H S, Xu P G, Zheng Y K. Heat Treat Met, 2001; 25(6) : 1(黄进峰,方鸿生,徐平光,郑燕康.金属热处理,2001;25(6) :1)
[6] Chen Y T, Fang H S, Bai B Z, Yan Z G, Li Q, Hou C Q, Gao F. Heat Treat Met, 2001; 26(8) : 5(陈颜堂,方鸿生,白秉哲,杨志剐,李琪,侯传基,高凡.金属热处理,2001;26(8) :5)
[7] Chu W Y. Hydrogen Induced Failure and Delayed Failure. Beijing: Metallurgy Industry Press, 1988:214(褚武扬.氢损伤和滞后断裂.北京:冶金工业出版社,1988:214)
[8] Fuchs H O. Stephens R I. Metal Fatigue in Engineering. New York: John Wiley & Sons. 1980:56
[9] ANSI. MIL-HDBK-5C (Military Material Handbook of America) Change Notice 2. Washington DC: ASTM. 1979
[10] Ritchie R O, Castrocedeno M H, Zackay V F, Parker E R. Met Trans A Phy Met Mater Sci, 1978; 9(1) : 35
[11] Berns H, Wener L. Theor Appl Frac Mech, 1986; (6) : 11
[12] Miihkinen V T T, Edmonds D V. Mater Sci Technol, 1987; 6:441
[1] DING Hua, ZHANG Yu, CAI Minghui, TANG Zhengyou. Research Progress and Prospects of Austenite-Based Fe-Mn-Al-C Lightweight Steels[J]. 金属学报, 2023, 59(8): 1027-1041.
[2] AN Xudong, ZHU Te, WANG Qianqian, SONG Yamin, LIU Jinyang, ZHANG Peng, ZHANG Zhaokuan, WAN Mingpan, CAO Xingzhong. Interaction Mechanism of Dislocation and Hydrogen in Austenitic 316 Stainless Steel[J]. 金属学报, 2021, 57(7): 913-920.
[3] SUN Chaofan CAI Qingwu WU Huibin MAO Hongyan CHEN Hongzhen. EFFECT OF CONTROLLED ROLLING PROCESSING ON NANOMETER–SIZED CARBONITRIDE OF Ti–Mo FERRITE MATRIX MICROALLOYED STEEL[J]. 金属学报, 2012, 48(12): 1415-1421.
[4] QIN Xiaomei CHEN Liqing DI Hongshuang DENG Wei. EFFECT OF DEFORMATION TEMPERATURE ON TENSILE DEFORMATION MECHANISM OF Fe-23Mn-2Al-0.2C TWIP STEEL[J]. 金属学报, 2011, 47(9): 1117-1122.
[5] ZHAO Shuai LI Xiuyan RONG Lijian. SERRATED FLOW IN A FeNi–BASED AUSTENITIC ALLOY[J]. 金属学报, 2011, 47(8): 1017-1021.
[6] WANG Yongwei XU Fengyun XU Xuexia BAI Bingzhe. RESEARCH ON TRANSFORMATION OF GRANULAR STRUCTURE IN LOW CARBON Mn–Si STEEL[J]. 金属学报, 2009, 45(5): 559-565.
[7] Xu Feng-yun. The influence of martensite volume fraction, shape and strength on the mechanical properties of granular structure steels[J]. 金属学报, 2008, 44(10): 1183-1187 .
[8] Xu Feng-yun. The phase transformation residual stress in granular structure[J]. 金属学报, 2008, 44(9): 1063-1068 .
[9] Jian ZHANG. EFFECTS OF GRAIN-BOUNDARY PHASES ON HYDROGEN EMBRITTLEMENT OF FE-NI-CR AUSTENITIC ALLOY BY INTERNAL FRICTION[J]. 金属学报, 2008, 44(9): 1095-1098 .
[10] GAO Jin. Corrosion Behavior of Microarc-oxidation Film on AZ91D Magnesium Alloy[J]. 金属学报, 2008, 44(8): 986-990 .
[11] ;. INVESTIGATION ON PHASE TRANSFORMATION OF ZG06Cr13Ni4Mo IN TEMPERING PROCESS WITH LOW HEATING RATE[J]. 金属学报, 2008, 44(6): 681-685 .
[12] Zhou Wen-Juan; Likun Xu; Jia Wang. study on corrosion electrochemical behavior of silane coating with flaked[J]. 金属学报, 2007, 43(9): 983-988 .
[13] WANG Songtao; YANG Ke; SHAN Yiyin; LI Laifeng. Effects of Cold Deformation on Microstructure And Mechanical Behavior of a High Nitrogen Austenitic Stainless Steel[J]. 金属学报, 2007, 43(7): 713-718 .
[14] . Effect of Hafnium on Radiation-induced Inter-granular Segregation in Ferritic Steel[J]. 金属学报, 2006, 42(10): 1041-1045 .
[15] Jian Zhang. STUDY OF HYDROGEN EMBRITLLEMENT IN Fe-Ni BASED ALLOY THROUGH POSITRON ANNIHILATION LIFETIME TEST[J]. 金属学报, 2006, 42(5): 469-473 .
No Suggested Reading articles found!