| Ferrite Transformation During Deformation of Undercooled Austenite in Low Carbon Steels with Different Mn Contents |
| zhou Rongfeng;YANG Wangyue; SUN Zuqing |
| School of Materials Science and Engineering;University of Science and Technology Beijing |
|
Cite this article:
zhou Rongfeng; YANG Wangyue; SUN Zuqing. Ferrite Transformation During Deformation of Undercooled Austenite in Low Carbon Steels with Different Mn Contents. Acta Metall Sin, 2004, 40(1): 1-7 .
|
|
|
Abstract The microstructure evolution during deformation of undercooled austenite
in three low carbon steels with much close contents of Si and C but
different contents of Mn has been investigated by means of hot
compression simulation experiment at 760℃ and strain rate of
1 s-1. The effects of the content of Mn on the deformed
behavior of undercooled austentie, the kinetics characteristics of
deformation enhanced ferrite transformation and the ferrite
grain size have been studied. It was found that the addition of Mn delays
the transformation during deformation of undercooled austenite and
higher true strain for the transformation is needed with increasing
Mn content. Transformation kinetics can be divided into three
stages, longer time and higher true strain are needed for each
stages with increasing Mn content in the steels. Deformation
enhanced transformation induces forming ultra--fine equiaxed ferrite
grains with sizes of 3.57±1.60, 2.00±1.05 and 2.29±1.02 um in steels with 0.48, 0.84 and 1.29 Mn respectively,
and homogeneously distributed minor second phases.
|
|
Received: 28 January 2003
|
|
|
[1] Yang W Y, Hu A M, Qi J J, Sun Z Q. Chin J Mater Res, 2001;15:171(杨王玥,胡安民,齐俊杰,孙祖庆.材料研究学报,2001;15:171) [2] Chiaki O, Tomoyoshi O, Takuzo I and Yasuhi U. Trans ISIJ, 1980; 20:833 [3] Tamura I, Sekine H, Tanaka T, Ouchi C. Trans by Wang G D, Liu Z Y, Xiong S W. Thermomechanical Processing of High Strength Low Alloy Steels. Beijing: Metallurgy Industry Press. 1992:89(Tamura I,Sekine H,Tanaka T著.王国栋,刘振宇,熊尚武译.高强度低合金钢的控制轧制与控制冷却.北京:冶金工业出版社.1992:89) [4] Yang W Y, Hu A M, Sun Z Q. Acta Metall Sin, 2000; 36: 1055(杨王玥,胡安民,孙祖庆.金属学报,2000;36:1055) [5] Qi J J. PhD Thesis, Univ Sci Technol Beijing, Beijing,2002(齐俊杰.北京科技大学博士学位论文.2002) [6] Aaronson H I. The Mechanism of Phase Transformation in Crystalline. London: Institute of Metals, 1969:2790 [7] Liu Y Q. Heat Treatment of Steel. Beijing: Metallurgy Industry Press. 1983:42(刘永铨.钢的热处理.北京:冶金工业出版社.1983:42) [8] Qi J J, Yang W Y, Sun Z Q. Acta Metall Sin, 2002; 38: 897(齐俊杰,杨王玥,孙祖庆.金属学报,2002;38:897) |