[1] Li S B, Zhang J X. Dev Appl Mater, 2001; 16(6): 39
(李少兵, 张俊旭. 材料开发与应用, 2001; 16(6): 39)
[2] Montemarano T W. J Ship Prod, 1986; 2: 145
[3] Wang S C, Kao P. J Mater Sci, 1993; 28: 5169
[4] Thompson S W, Krauss G. Metall Trans, 1996; 27A: 1573
[5] Ren H P, Liu Z C, Wang H Y, Guo F L. Trans Mater Heat Treat, 2007; 28(suppl): 119
(任慧平, 刘宗昌, 王海燕, 郭凤莲. 材料热处理学报, 2007; 28(增刊): 119)
[6] Avazkonandeh M H, Haddad M, Haerian A. Mater Des, 2009; 30: 1902
[7] Babu S S. Curr Opin Solid State Mater Sci, 2004; 8: 67
[8] Farrar R A, Harrison P L. J Mater Sci, 1987; 22: 12
[9] Wang W, Liu S. Weld J, 2002; 81(7): 132
[10] Widgery D J. Met Constr, 1978; 10: 480
[11] Shackleton D. British Weld J, 1967; 1: 592
[12] Morito S, Tanaka H, Konishi H, Furuhara T, Maki T. Acta Mater, 2003; 6: 1789
[13] Singh S B, Bhadeshia H K. Mater Sci Eng, 1998; A245: 72
[14] Xue G, Zhang J H, Yao R G. China Weld, 2007; 16(1): 31
[15] Li S B, Zhang J X, Zhu B K. Weld Join, 2005; (11): 27
(李少兵, 张俊旭, 朱炳坤. 焊接, 2005; (11): 27)
[16] Essouni M, Beaven P A. Mater Sci Eng, 1990; S130: 173
[17] Hehemann A F, Kinsman K, Aaronson H I. Metall Trans, 1972; 5: 1077
[18] Yi H L, Ma Q S, Du L X, Lin X H, Wang G D. Mater Mech Eng, 2009; 33(6): 37
(衣海龙, 麻庆申, 杜林秀, 刘相华, 王国栋. 机械工程学报, 2009; 33(6): 37)
[19] Song W X. Metallography. Beijing: Metallurgy Industry Press, 2008: 374
(宋微锡. 金属学. 北京: 冶金工业出版社, 2008: 374)
[20] Gao X L, Fu G Q, Deng Z Y, Lin G M, Zhu M Y. Chin JProcess Eng, 2010; 10: 998
(高新亮, 付贵勤, 邓志银, 林光铭, 朱苗勇. 过程工程学报, 2010; 10: 998)
[21] Onck P R, Andrews E W, Gibson L J. Int J Mech Sci, 2001; 43: 681
[22] Zhang Y Q, Zhang R J, Su H, Li L. Iron Steel, 2003; 38: 45
(张永权, 张荣久, 苏航, 李丽. 钢铁, 2003; 38: 45)
[23] Hwang B, Kin Y G, Lee S, Kim Y M, Kim N J, Yoo J Y. Metall Mater Trans, 2005; 36A: 2107
[24] Zhao L, Zhang X D, Chen W Z. Acta Metall Sin, 2005; 41: 392
(赵 琳, 张旭东, 陈武柱. 金属学报, 2005; 41: 392)
[25] Bonnevie E, Ferri`ere G, Ikhlef A. Mater Sci Eng, 2004; A385: 352
[26] Davis C L, King J E. Mater Sci Technol, 1993; 9: 8
[27] Ju D C, Zhu P X, Yan H C, Liu J Q. Metall Collect, 2008; (2): 41
(居殿春, 竺培显, 颜慧成, 刘家琪. 冶金丛刊, 2008; (2): 41)
[28] Cui Z Q. Metallography and Heat Treatment. Beijing: China Machine Press, 1999: 39
(崔忠圻. 金属学与热处理. 北京: 机械工业出版社, 1999: 39)
[29] Fang H S, Wang J J, Yang Z G, Li C M, Bo X Z, Zheng Y K. Bainite Transformation. Beijing: Science Press, 1999: 370
(方鸿生, 王家军, 杨志刚, 李春明, 薄详正, 郑燕康. 贝氏体相变.北京: 科学出版社, 1999: 370)
[30] Xu Z, Zhao L C. Transformation Theory of Metal in Solid. Beijing: Science Press, 2004: 120
(徐 洲, 赵连城. 金属固态相变原理. 北京: 科学出版社, 2004: 120)
[31] Diazfuentes M, Izamendia A, Gutierrez I. Metall Mater Trans, 2003; 34A: 2005
[32] Sa S Y, Wang P. Chin J Nonferrous Met, 2010; 20(Spec.): 429
(撒世勇, 王平. 中国有色金属学报, 2010; 20(特刊): 429) |