Abstract The corrosion behaviors of low alloy steel P265GH and carbon steel Q235 deposited with NaCl and NaHSO3 under dry/humid alternative condition were investigated by FTIR, XRD, SEM and galvanostatic method. The results reveal that under present experimental condition, corrosion rates of low alloy steel and carbon steel decrease with prolonging time and their mass losses are almost identical. Besides, corrosion resistance of low alloy steel P265GH is not better than that of carbon steel Q235. The corrosion products formed on the two steels are mainly composed of δ-FeOOH, α-FeOOH, Fe3O4, γ-FeOOH and sulphate, among which δ-FeOOH is predominant. The existence of δ-FeOOH accounts for the decrease of corrosion rates of the steels.
|
|
Received: 20 May 2010
|
| Fund: Supported by Science and Technology Plan Project of Shenyang (No.1091182-1-00) |
| 参考文献
[1] Singh D D N, Yadav S, Saha J K. Corros Sci, 2008; 50: 93
[2] Casta?o J G, Botero C A, Restrepo A H, Agudelo E A, Correa E, Echeverría F. Corros Sci, 2010; 52: 216
[3] Ma Y T, Ying Li, Wang F H. Corros Sci, 2009; 51: 997
[4] Qu Q, Yan C W, Zhang L, Yan Y G, Wan Y, Cao C N. The Chinese journal of Nonferrous Metals, 2002; 12: 1272
(曲庆, 严川伟, 张蕾, 阎一功, 万晔, 曹楚南. 中国有色金属学报, 2002; 12: 1272)
[5] Qu Q, Yan C W, Cao C N. CORROSION SCIENC AND PROTECTION TECHNOLOGY, 2001; 13: 432
(曲庆, 严川伟, 曹楚南. 腐蚀科学与防护技术, 2001; 13: 432)
[6] Ma Y T, Li Y, Wang F H. Materials Chemistry and Physics, 2008; 06: 066
[7] Qu Q, Yan C W, Bai W, Cao C N. ACTA METALLURGICA SINICA, 2001; 37: 72
(曲庆, 严川伟, 白玮, 曹楚南. 金属学报, 2001; 37: 72)
[8] Qu Q, Yan C W, Zhang L, Wan Y, Cao C N. ACTA METALLURGICA SINICA, 2002; 38: 1062
(曲庆, 严川伟, 张蕾, 万晔, 曹楚南. 金属学报, 2002; 38: 1062)
[9] Wang Z Y, Zheng Y P, Liu S R. JOURNAL OF CHINESE SOCIETY FOR CORROSION AND PROTECTION, 1994; 14: 240
(王振尧, 郑逸萍, 刘寿荣. 中国腐蚀与防护学报, 1994; 14: 240)
[10] Wang Z Y, Yu G C, Han W. CORROSION SCIENCE AND PROTECTION TECHNOLOGY, 2004; 16: 70
(王振尧, 于国才, 韩薇. 腐蚀科学与防护技术, 2004; 16: 70)
[11] Misawa T, Kyuno T, Su?taka W, Shimodaira S. Corros Sci, 1971; 11: 35
[12] Raman A, Kuban B, Razvan A. Corros Sci, 1991; 32: 1295
[13] Yamashita M, Konishi H, Kozakura T, Mizuki J, Uchida H. Corros Sci, 2005; 47: 2492
[14] Misawa T, Asami K, Hashimoto K, Shimodaira S. Corros Sci, 1974; 14: 279
[15] Nishimura T, Katayama H, Noda K, Kodama T. CORROSION, 2000; 56: 935
[16] Keiser J T, Brown C W. Corros Sci, 1983; 23: 251
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|