INFLUENCE OF CERTAIN ALLOYING ELEMENTS ON THE CREEP ACTIVATION ENERGY OF PLATINUM
Ning Yuantao;Wang Yongli Institute of Noble Metals Research
Cite this article: 

Ning Yuantao;Wang Yongli Institute of Noble Metals Research. INFLUENCE OF CERTAIN ALLOYING ELEMENTS ON THE CREEP ACTIVATION ENERGY OF PLATINUM. Acta Metall Sin, 1979, 15(4): 548-594.

Download:  PDF(1306KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The influence of certain alloying elements such as Rh, Au, Mo, W, Zr andHf on the activation energy of creep of platinum alloys at high temperatures hasbeen investigated. The presence of Rh, Zr or/and Hf in the alloys might causean increment of their activation energy of creep but W, Mo or/and Au mightdecrease them. Based on the behaviour of these alloying elements, the mechanismof the creep rupture of the platinum alloys has been discussed.
Received:  18 April 1979     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1979/V15/I4/548

[1] Bennett, H. E., Platinum Metals Rev., 2 (1958) , 120.
[2] Bourne, A. A. and Darling, A. S., Platinum Metals Rev., 7 (1963) , 42.
[3] Reinacher, G., Metall., 15 (1961) , 657; 29 (1975) , 681.
[4] Sadowski, E. P., Refract. Metals Alloys, 11 (1960) , 465.
[5] Darling, A. S., Platinum Metals Rev.. 17 (1973) , 130.
[6] 38 (1974) , 4, 827.
[7] 1977, 169.
[8] 37(1974) , 1, 142.
[9] Chaston, J. C., Platinum Metals Rev., 19 (1975) , 135.
[10] Owens-Corning Fiberglass Corp., U. S. Pat. 3, 622, 289, 1972.
[11] Owens-Corning Fiberglass Corp., Brit. Pat. 1,350, 644, 1974.
[12] Conrad, H., High-Strength Materials, Ed. by V. F. Zackay, Wiley, New York, 1965, p. 445.
[13] Reinacher, G., Z. Metallk., 62 (1971) , 835.
[14] Selman, G. L., Day, J. G. and Bourne, A. A., Platinum Metals Rev., 18 (1974) , 42; 20 (1976) , 86.:
No related articles found!
No Suggested Reading articles found!