Abstract The free energy calculation of the interaction between molybdenum and theoxides in glasses has been correlated with the results obtained by immersing mol-ybdenum electrodes in molten glass bath in work's practice. The corrosion rateof molybdenum electrode as observed was directly proportional to the currentdensity and to the temperature of molten glass, the critical current density beingabout 0.4-0.7 A/cm~2. After one year's service in molten glass, the structure ofmolybdenum became very coarsely recrystallized, with an oxygen content of 0.04to 0.38 wt% (max). It would appear therefore, that molybdenum is sufficientlycorrosion-resistant to be adequately used as electrode or as structural materials inglass industry.
|
|
Received: 18 April 1979
|
[1] Stanek, J., Electric Melting of Glass, Elsevier, Amsterdam, 1977, p. 334. [2] 吾妻洁,亀田满雄,冶金物理化学--制錬基礎论,朝仓书店,1964,p,76. [3] Elliott, J. F., Gleiser, M. and. Ramakrishna, V., Thermochemistry for Steelmaking, vol. Ⅱ, American Iron and Steel Institute, 1963, p. 617. [4] 大冈一夫,窑业协协会志, 76 (1964) ,№ 824,108. [5] Kahl, W., Silikattenchnik, 3 (1978) , 76. [6] Vobornik, K., Silikat-Journal, 8 (1969) , 162. [7] Kubaschewski, O. and Evans, E. LL., Metallurgical Thermochemistry, Pergamon Press, London, 1958, p. 260.@ |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|