EFFECT OF RARE EARTH ADDITIONS ON THE IMPACT FRACTURE OF Cr18Nil8Si2 STEEL
Qiu Jufeng;Cheng Wanrong Baotou Metallurgical Institute
Cite this article: 

Qiu Jufeng;Cheng Wanrong Baotou Metallurgical Institute. EFFECT OF RARE EARTH ADDITIONS ON THE IMPACT FRACTURE OF Cr18Nil8Si2 STEEL. Acta Metall Sin, 1979, 15(4): 557-596.