| HYDROGEN INDUCED INTERGRANULAR CLEAVAGE IN Fe-3%Si ALLOY |
| WANG Yanbin CHU Wuyang XIAO Jimei (Beijing University of Iron and Steel Technology) |
|
Cite this article:
WANG Yanbin CHU Wuyang XIAO Jimei (Beijing University of Iron and Steel Technology). HYDROGEN INDUCED INTERGRANULAR CLEAVAGE IN Fe-3%Si ALLOY. Acta Metall Sin, 1987, 23(1): 89-91.
|
|
|
Abstract Single notched specimens,charged dynamically with hydrogen,were tested under ten- sion.It was shown that the hydrogen induced crack is propagated macroscopically along the grain boundary,but the fracture is revealed on fraetograph as along the cleavage planes immediately vicinal to the grain boundary.It seems to explain the above mentioned hardly by tde decohesive theory other than the mechanism of hydrogen facilitated cleavage pro- posed by the authors.
|
|
Received: 18 January 1987
|
1 Beachem C D.Metall Trans,1972;3:437 2 Chu W Y(褚武扬),Li S Q(李世琼),Hsiao C M(肖纪美)et al.Corrosion,1980;36:475 3 Chu W Y(褚武扬),Hsiao C M(肖纪美),Li W X(李文学)et al.Metall Trans,1984;15A:2087 4 Yoshino K,McMahon C J Jr.Metall Trans,1974;5:363 5 Robertson I M,Tabata T,Wei W,et al.Sct Metall,1984;18:841 6 Wang Y B(王燕斌),Chu W Y(褚武扬),Hsiao C M(肖纪美),Scr Metall,1986;19:116 7 张统一,褚武扬,肖纪美.中国科学 A.1986;(3) :316 8 Wang Y B(王燕斌),Chu W Y(褚武扬),Hsiao C M(肖纪美).Scr Metall,1986;19:1157 9 Oriani R A.Josephic P H.Acta Metall,1977;25:979 10 Hirth J P.Metall Trans,1980;11A:861 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|