Abstract  From experimental or theoretical aspect,three Euler indices of a polyhedral grain are equal statistically to the mean caliper diameter of the same grain,when all the values of the foresaid parameters being normalized respectively by their average in the space filling polycrystal to which the grain belongs.It seems that the above principle is independent of the type of the metal concerned,provide that the structures are configured in a way that is consistent with the underlying assumption in the derivation of the principle.
Received:  18 January 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I1/86

1 Desch C.J Inst Met,1919;22:241
2 Williams W M,Smith C S.Trans AIME 1952;194:755
3 Okazaki K,Conrad H.Trans Jpn Inst Met,1972;13:198
4 Rhines F N,Patterson B R.Metall Trans 1982;13A:985
5 Liu G Q(刘国权).Ph.D Dissertation.Univ.of Florida,Gainesville FL,1984
6 DeHoff R T,Liu G Q(刘国权).Metall Trans,1985;16A:2007.
7 Smith C S.In:Metal Interfaces,Cleveland:ASM,1952,65E
No related articles found!
No Suggested Reading articles found!