EFFECT OF HYDROGEN ON DISLOCATION VELOCITY-STRESS EXPONENTS OF Ti ALLOYS
CAO Mingzhou YANG Ke WAN Xiaojing (Institute of Metal Research;Academia Sinica;Shenyang)
Cite this article: 

CAO Mingzhou YANG Ke WAN Xiaojing (Institute of Metal Research;Academia Sinica;Shenyang). EFFECT OF HYDROGEN ON DISLOCATION VELOCITY-STRESS EXPONENTS OF Ti ALLOYS. Acta Metall Sin, 1987, 23(1): 92-94.

Download:  PDF(210KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The dislocation velocity-stress exponents,m~*,of commercial pure Ti,Ti-6Al-4V and Ti-15Mo alloys,which were charged with hydrogen,were measured by means of the stress relaxation method at room temperature.The results show that when hydrogen concentration in pure Ti,Ti-6Al-4V and Ti-15Mo alloys exceeds 310,620 and 1100 ppm respectively, the m~* value increases as the increasing of hydrogen concentration,that seems to be due to decreasing the binding energy of lattice.
Received:  18 January 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I1/92

1 Johnston W J,Gilman J J.J Appl Phys.1959;30:129
2 Li J C M.Can J Phys.1967;45;493
3 尹万全,苏会和,徐永波,秦荣士,刘民治.金属学报,1985;21:A323
4 Troiano A R.Trans ASM,1960;52:54
5 万暁景,杨柯,曹名洲.金属学报,1986;22:189
6 Tien J K.Metall Trans,1976;7A:821h
No related articles found!
No Suggested Reading articles found!