CRYSTAL LATTICES OF SmPd_5 AND EuPd_5
ZHANG Kanghou;CHEN Lili Institute of Precious Metals; Kunming
Cite this article: 

ZHANG Kanghou;CHEN Lili Institute of Precious Metals; Kunming. CRYSTAL LATTICES OF SmPd_5 AND EuPd_5. Acta Metall Sin, 1988, 24(1): 135-137.

Download:  PDF(190KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Single phase compounds SmPd_5 and EuPd_5 have been prepared respectively X-raydiffraction has been used to determine the structure and lattice parameters. Both of them exhibita SmPt_5-type structure. Following lattice parameters have been obtained:α=0.5253nm, b=0.9015nm, c=2.568nm for SmPd_5;α=0.5268nm, b=0.8984nm, c=2.553nm for EuPd_5.
Key words:  intermetallic compound SmPd_5      EuPd_5      X-ray diffraction      crystal lattice     
Received:  18 January 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I1/135

1 Loebich O Jr., Raub E. J Less-Common Met, 1973; 30: 47
2 Jordan R G, Loebich O Jr. J Less-Common Met, 1975; 39: 55
3 Iandelli A, Palenzina A. J Less-Common Met, 1974; 38: 1
4 #12
5 陈念贻,谢雷鸣,施天生,江乃雄,李庆兰.中国科学,1981;(7) :836
6 Bronger W. J Less-Common Met. 1967; 12: 63
7 Iandelli A, Palenzona A. J Less-Common Met, 1981; 80: 71
8 #12)
[1] LI Shilei, LI Yang, WANG Youkang, WANG Shengjie, HE Lunhua, SUN Guang'ai, XIAO Tiqiao, WANG Yandong. Multiscale Residual Stress Evaluation of Engineering Materials/Components Based on Neutron and Synchrotron Radiation Technology[J]. 金属学报, 2023, 59(8): 1001-1014.
[2] LI Yizhuang,HUANG Mingxin. A Method to Calculate the Dislocation Density of a TWIP Steel Based on Neutron Diffraction and Synchrotron X-Ray Diffraction[J]. 金属学报, 2020, 56(4): 487-493.
[3] LI Changji,ZOU Minjie,ZHANG Lei,WANG Yuanming,WANG Sucheng. High-Resolution X-Ray Diffraction Analysis of Epitaxial Films[J]. 金属学报, 2020, 56(1): 99-111.
[4] Weifeng HE, Xiang LI, Xiangfan NIE, Yinghong LI, Sihai LUO. Study on Stability of Residual Stress Induced by Laser Shock Processing in Titanium Alloy Thin-Components[J]. 金属学报, 2018, 54(3): 411-418.
[5] Yutuo ZHANG,Cong LI,Pei WANG,Dianzhong LI. IN SITU SYNCHROTRON X-RAY DIFFRACTION INVESTIGATION ON TENSILE PROPERTIES OF 9Ni STEEL[J]. 金属学报, 2016, 52(4): 403-409.
[6] Shenghua ZHANG,Pei WANG,Dianzhong LI,Yiyi LI. INVESTIGATION OF TRIP EFFECT IN ZG06Cr13Ni4Mo MARTENSITIC STAINLESS STEEL BY IN SITU SYNCHROTRON HIGH ENERGY X-RAY DIFFRACTION[J]. 金属学报, 2015, 51(11): 1306-1314.
[7] Zhao Ning. THE LIQUID STRUCTURE OF SN-CU LEAD-FREE SOLDERS[J]. 金属学报, 2008, 44(4): 467-472 .
[8] JIANG Chuanhai; WU Jiansheng; WANG Dezun. X--Ray Diffraction Analysis for the Recrystallization Behavior Of SiCw/Al Composite at High Temperature[J]. 金属学报, 2004, 40(10): 1023-1026 .
[9] WANG Huabin; HAN Jiecai; ZHANG Xinhong; DU Shanyi (Center for Composite Materials; Harbin Institute of Technology; Harbin 150001)Correspondent: WANG Huabin; lecturer;Tel: (0451)6414167; Fax: (0451)6415605. REACTION MECHANISM OF CONTINUALLY HEATING Ni AND A1 PARTICLES[J]. 金属学报, 1998, 34(9): 992-998.
[10] PAN Hongge; DU Honglin; CHEN Changpin; HAN Xiufeng; YANG Fuming (Department of Materials Science and Engineering; Zhejiang University; Hangzhou 310027)(State Key Laboratory for Magnetism; Institute of Physics; The Chinese Academy of Sciences; Beijing 100080)(Institute of Chinese Atomic Energy; Beijing 102413). STRUCTURAL CHARACTERIZATION OF THE Y_3(Fe, Mo)_(29) INTERMETALLIC COMPOUND[J]. 金属学报, 1998, 34(5): 473-482.
[11] LEI Yongquan;ZHANG Wenkui;YANG Xiaoguang;WANG Qidong (Department of Materials Science and Engineering; Zhejiang University; Hangzhou 310027)LU Guanglie (Central Laboratory; Hangzhou University; Hangzhou 310028). PHASE COMPOSITION OF ZrM_2(M=Mn, V, Ni)HYDROGEN STORAGE ALLOYS[J]. 金属学报, 1998, 34(1): 45-50.
[12] WANG Fengping;WANG Peixuan;FANG Zhengzhi (University of Science and Technology Beting; Beting 100083); CUI Mingqi;JIANG Xiaoming; MA Hong; (Institute of High Energy Physics; Chinese Academy of Sciences; Beijing 100039). THE INTERFACIAL ANALYSIS OF MO/SiO_2 MULTILAYERS MIRROR FOR SOFT X-RAY[J]. 金属学报, 1997, 33(7): 737-741.
[13] YIN Xiaoying;WANG Yingang;TANG Ning;YANG Fuming(State Key Laboratory of Magnetism; Institute of Physics; Chinese Academy of Sciences; Beijing 100080)(Chinese People's Public Security University; Beijing 100038). CRYSTAL STRUCTURE AND MAGNETIC PROPERTIES OF Y_2Fe_(17-x)Mn_x[J]. 金属学报, 1997, 33(5): 539-542.
[14] WANG Fengping;CUI Mingqi; WANG Peixuan; FANG Zhengzhi University; of Science and Technology Beijing; Beijing 100083 Institute of High Energy Physics; Chinese Academy of Sciences; Beijing 100039(Manuscript received 1995-10-04). STUDY OF MULTILAYER INTERFACE ROUGHNESS BY LOW-ANGLE X-RAY DIFFRACTION[J]. 金属学报, 1996, 32(7): 774-778.
[15] GAI Hiuying; LI Jiabao; KANG Zengqiao; WANG Zhongguang (State Key Laboratory for Fatigue and Fracture of Materials;Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)ZHU Yongping; LI Chao (Shenyang Polytechnical University; Shenyang 110023). MECHANICAL PROPERTIES OF SHOT PEENED SURFACE FOR STEEL 60Mn[J]. 金属学报, 1996, 32(6): 605-610.
No Suggested Reading articles found!