| CRYSTAL LATTICES OF SmPd_5 AND EuPd_5 |
| ZHANG Kanghou;CHEN Lili Institute of Precious Metals; Kunming |
|
Cite this article:
ZHANG Kanghou;CHEN Lili Institute of Precious Metals; Kunming. CRYSTAL LATTICES OF SmPd_5 AND EuPd_5. Acta Metall Sin, 1988, 24(1): 135-137.
|
|
|
Abstract Single phase compounds SmPd_5 and EuPd_5 have been prepared respectively X-raydiffraction has been used to determine the structure and lattice parameters. Both of them exhibita SmPt_5-type structure. Following lattice parameters have been obtained:α=0.5253nm, b=0.9015nm, c=2.568nm for SmPd_5;α=0.5268nm, b=0.8984nm, c=2.553nm for EuPd_5.
|
|
Received: 18 January 1988
|
1 Loebich O Jr., Raub E. J Less-Common Met, 1973; 30: 47 2 Jordan R G, Loebich O Jr. J Less-Common Met, 1975; 39: 55 3 Iandelli A, Palenzina A. J Less-Common Met, 1974; 38: 1 4 #12 5 陈念贻,谢雷鸣,施天生,江乃雄,李庆兰.中国科学,1981;(7) :836 6 Bronger W. J Less-Common Met. 1967; 12: 63 7 Iandelli A, Palenzona A. J Less-Common Met, 1981; 80: 71 8 #12) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|