THERMODYNAMICS OF TERNARY Fe-B-Si MELTS AT 1450℃ Ⅱ. ACTIVITY OF B AND ITS INTERACTION COEFFICIENTS
JI Chunlin;YU Rongxiang Northeast University of Technology;LIU Sulan Leeturer;Department of Metallurgtcal Physicat Chemistry;Northeast University of Technotogy;Shenyang
Cite this article: 

JI Chunlin;YU Rongxiang Northeast University of Technology;LIU Sulan Leeturer;Department of Metallurgtcal Physicat Chemistry;Northeast University of Technotogy;Shenyang. THERMODYNAMICS OF TERNARY Fe-B-Si MELTS AT 1450℃ Ⅱ. ACTIVITY OF B AND ITS INTERACTION COEFFICIENTS. Acta Metall Sin, 1988, 24(2): 161-165.

Download:  PDF(321KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  To calculate the activity coefficient In γ_j in ternary Fe-i-j systems,a method of Gibbs-Duhem intergration using available data of ln γ_i with no extraneed of any binary data has been proposed. Activity coefficient of B and relevantinteraction coefficients have been derived by means of this method with In γ_(Si) valuedetermined experimentally in the part I of the present work: lnγ°B=-2.82,ε_B~B=5.7,ρ_B~B=-2.8l,ε_B~(Si)=16.0 ρ_B~(Si)=24.7 and ρ_B~(B,Si)=-34.3
Key words:  Fe-B-Si system      activity      activity coefficient      activity interaction coefficient      sequential method     
Received:  18 February 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I2/161

1 Darken L S. J Amer Chem Soc, 1950; 72: 2909
2 Wagner C. Thermodynamics of Alloys, Reading Mass: Addison-Wesley, 1952: 19
3 Makay H A C. Trans Faraday Soc, 1953; 49: 237
4 Schuhmann R Jr. Acta Metall, 1955; 3: 219
5 Gokcen N A. J Phys Chem, 1960; 64: 401
6 周国治.中国科学,1977;(5) :456
7 王之昌,周国治.中国科学,1984;(10) :959
8 冀春霖,俞荣祥,刘素兰.金属学报,1988;24:B87
9 Evans D B. Pehlke R D. Trans Metall Soc AIME. 1964; 230. 1657
10 Ball D L. Trans Metall Soc AIME, 1967; 239: 31
11 Schenck H, Steinmetz E. Arch Eisenhuettenwes, 1968; 39: 255
12 Fruehan R J. Metall Trans, 1970; 1: 2083
13 Lupis C H P, Elliott J F. Acta Metall, 1966; 14: 529
14 Darken L S. Trans Metall Soc AIME, 1967; 239: 80
[1] JU Tianhua, SHU Nian, HE Wei, DING Xueyong. A Predicted Model for Activity Interaction Coefficient Between Solutes in Alloy Solutions[J]. 金属学报, 2023, 59(11): 1533-1540.
[2] Rongyao MA, Lin ZHAO, Changgang WANG, Xin MU, Xin WEI, Junhua DONG, Wei KE. Influence of Hydrostatic Pressure on the Thermodynamics and Kinetics of Metal Corrosion[J]. 金属学报, 2019, 55(2): 281-290.
[3] Xiaofeng LU, Ming XIAO, Yangmei CHEN, Bangcheng YANG. Bioactivity of Titanium Metal Hybridized with Inactivated Bacterial Biofilm[J]. 金属学报, 2017, 53(10): 1402-1412.
[4] Muqin LI, Haitao YAO, Fanghong WEI, Mingda LIU, Zan WANG, Shuhao PENG. The Microstructure and in Vivo and in Vitro Property of Multi-Component Composite Films on the Biomedical Pure Magnesium Surface[J]. 金属学报, 2017, 53(10): 1337-1346.
[5] Xiaoyan CHEN,Zhe JIN,Xuefeng BAI,Yizhou ZHOU,Tao JIN,Xiaofeng SUN. EFFECT OF C ON THE INTERFACIAL REACTION AND WETTABILITY BETWEEN A Ni-BASED SUPERALLOY AND CERAMIC MOULD[J]. 金属学报, 2015, 51(7): 853-858.
[6] Dongsong RONG,Yong JIANG,Jianming GONG. EXPERIMENTAL RESEARCH AND THERMODYNAMIC SIMULATION OF LOW TEMPERATURE COLOSSAL CARBURIZATION OF AUSTENITIC STAINLESS STEEL[J]. 金属学报, 2015, 51(12): 1516-1522.
[7] WU Ling. The improvement of regular solution model based on GA-NN and its application in binary slag system[J]. 金属学报, 2008, 44(7): 799-802 .
[8] Yuan Liu. Improvement of Calculation Method for the Activity Coefficient of Multi-component Alloys[J]. 金属学报, 2007, 43(5): 503-508 .
[9] LE Qichi; CUI Jianzhong. Thermodynamics Properties of Ternary Bath of Coloring Hot--Dip Galvanization[J]. 金属学报, 2006, 42(11): 1182-1186 .
[10] MA Zhongting; J. OHSER; D. JANKE(The Institute of Iron and Steel Technology; Freiberg University of Mining and Technology; Freiberg; Germany). THERMODYNAMIC DESCRIPTION OF MULTICOMPONENT SYSTEMS BY INTERACTION MRAMETERS[J]. 金属学报, 1998, 34(7): 753-762.
[11] LUO Lihua; DING Xueyong; GUO Dan; CAO Wenbin; ZOU Zongshu; WANG Wenzhong (School of Materials and Metallurgy; Northeastern University; Shenyang 110006)( University of Science and Technology Beijing; Beijing 1100083). DATABASE SOFTWARE DEVELOPMENT FOR ACTIVITY AND INTERACTION MRAMETER OF ALLOY SYSTEMS[J]. 金属学报, 1998, 34(4): 388-392.
[12] ZHANG Ziqing(Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015). DISCUSSION ON THE METHOD TO DETERMINE THE ACTIVITY IN SLAGS BY MEANS OF THE SLAGMETAL EQUILIBRIA IN A LIQUID STATE[J]. 金属学报, 1998, 34(3): 299-304.
[13] CHEN Erbao; DONG Yuanchi; GUO Shangxing (EaSt China Institute of Metallurgy; Ma'anshan 243002) (Manuscript received 1996-09-15; in revised form 1996-11-25). STUDY ON THERMODYNAMICAL PROPERTIES IN Mn-Fe ALLOY MELTS[J]. 金属学报, 1997, 33(8): 831-837.
[14] ZHANG Jian (University of Science and Technology Beijing; Beijing 100083). CALCULATING MODELS OF MASS ACTION CONCENTRATIONS FOR SEVERAL MOLTEN BINARY SALTS[J]. 金属学报, 1997, 33(5): 515-523.
[15] ZHANG Xiaobing;JIANG Guochang;XU Kuangdi (Shanghai University; ShanghaiEnhanced Lab of Ferrometallurgy; Shanghai 200072). HIGH ORDER SUB-REGULAR SOLUTION MODEL AND ITS APPLICATIONS IN THE CALCULATION OF COMPONENT ACTIVITIES OF MnO-SiO_2-Al_2O_3-CaO MOLTEN SLAG[J]. 金属学报, 1997, 33(10): 1085-1093.
No Suggested Reading articles found!