VAPOUR PRESSURE OF Sb AND ACTIVITIES IN LIQUID Cu-Sb ALLOYS
LIU Xiangjun Lecturer;Department of Chemistry;Beijing University of Iron and Steel Technology;TAN Guoliang;MAO Yuwen;WANG Jian Beijing University of Iron and Steel Technology
Cite this article: 

LIU Xiangjun Lecturer;Department of Chemistry;Beijing University of Iron and Steel Technology;TAN Guoliang;MAO Yuwen;WANG Jian Beijing University of Iron and Steel Technology. VAPOUR PRESSURE OF Sb AND ACTIVITIES IN LIQUID Cu-Sb ALLOYS. Acta Metall Sin, 1988, 24(2): 166-170.

Download:  PDF(385KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The vapour pressure of Sb in liquid Cu-Sb alloys (x_(sb)=0.262--0.815)were measured at 820--1060K by means of torsion effusion method. Activities ofSb were calculated from the obtained data and those of Cu by Gibbs-Duhem inter-gration. Problems about the experimental techniques have also been discussed.
Key words:  vapour pressure      Cu-Sb alloys      activity      torsion effusion method     
Received:  18 February 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I2/166

1 #12
2 #12
3 阿座上竹四,矢沢彬,日本鉱业会志,1967;83(948) :666
4 Kubaschewski O. Metallurgical Thermochemistry, Sth ed., Vol. 24, New York: Pergamon Press, 1979: 364
5 Hultgren R. Selected Values of the Thermodynamic Properties of the Elements, Metals Park, Ohio: ASM, 1973: 448
[1] JU Tianhua, SHU Nian, HE Wei, DING Xueyong. A Predicted Model for Activity Interaction Coefficient Between Solutes in Alloy Solutions[J]. 金属学报, 2023, 59(11): 1533-1540.
[2] Rongyao MA, Lin ZHAO, Changgang WANG, Xin MU, Xin WEI, Junhua DONG, Wei KE. Influence of Hydrostatic Pressure on the Thermodynamics and Kinetics of Metal Corrosion[J]. 金属学报, 2019, 55(2): 281-290.
[3] Xiaofeng LU, Ming XIAO, Yangmei CHEN, Bangcheng YANG. Bioactivity of Titanium Metal Hybridized with Inactivated Bacterial Biofilm[J]. 金属学报, 2017, 53(10): 1402-1412.
[4] Muqin LI, Haitao YAO, Fanghong WEI, Mingda LIU, Zan WANG, Shuhao PENG. The Microstructure and in Vivo and in Vitro Property of Multi-Component Composite Films on the Biomedical Pure Magnesium Surface[J]. 金属学报, 2017, 53(10): 1337-1346.
[5] Xiaoyan CHEN,Zhe JIN,Xuefeng BAI,Yizhou ZHOU,Tao JIN,Xiaofeng SUN. EFFECT OF C ON THE INTERFACIAL REACTION AND WETTABILITY BETWEEN A Ni-BASED SUPERALLOY AND CERAMIC MOULD[J]. 金属学报, 2015, 51(7): 853-858.
[6] Dongsong RONG,Yong JIANG,Jianming GONG. EXPERIMENTAL RESEARCH AND THERMODYNAMIC SIMULATION OF LOW TEMPERATURE COLOSSAL CARBURIZATION OF AUSTENITIC STAINLESS STEEL[J]. 金属学报, 2015, 51(12): 1516-1522.
[7] WU Ling. The improvement of regular solution model based on GA-NN and its application in binary slag system[J]. 金属学报, 2008, 44(7): 799-802 .
[8] Yuan Liu. Improvement of Calculation Method for the Activity Coefficient of Multi-component Alloys[J]. 金属学报, 2007, 43(5): 503-508 .
[9] LE Qichi; CUI Jianzhong. Thermodynamics Properties of Ternary Bath of Coloring Hot--Dip Galvanization[J]. 金属学报, 2006, 42(11): 1182-1186 .
[10] MA Zhongting; J. OHSER; D. JANKE(The Institute of Iron and Steel Technology; Freiberg University of Mining and Technology; Freiberg; Germany). THERMODYNAMIC DESCRIPTION OF MULTICOMPONENT SYSTEMS BY INTERACTION MRAMETERS[J]. 金属学报, 1998, 34(7): 753-762.
[11] LUO Lihua; DING Xueyong; GUO Dan; CAO Wenbin; ZOU Zongshu; WANG Wenzhong (School of Materials and Metallurgy; Northeastern University; Shenyang 110006)( University of Science and Technology Beijing; Beijing 1100083). DATABASE SOFTWARE DEVELOPMENT FOR ACTIVITY AND INTERACTION MRAMETER OF ALLOY SYSTEMS[J]. 金属学报, 1998, 34(4): 388-392.
[12] ZHANG Ziqing(Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015). DISCUSSION ON THE METHOD TO DETERMINE THE ACTIVITY IN SLAGS BY MEANS OF THE SLAGMETAL EQUILIBRIA IN A LIQUID STATE[J]. 金属学报, 1998, 34(3): 299-304.
[13] CHEN Erbao; DONG Yuanchi; GUO Shangxing (EaSt China Institute of Metallurgy; Ma'anshan 243002) (Manuscript received 1996-09-15; in revised form 1996-11-25). STUDY ON THERMODYNAMICAL PROPERTIES IN Mn-Fe ALLOY MELTS[J]. 金属学报, 1997, 33(8): 831-837.
[14] ZHANG Jian (University of Science and Technology Beijing; Beijing 100083). CALCULATING MODELS OF MASS ACTION CONCENTRATIONS FOR SEVERAL MOLTEN BINARY SALTS[J]. 金属学报, 1997, 33(5): 515-523.
[15] ZHANG Xiaobing;JIANG Guochang;XU Kuangdi (Shanghai University; ShanghaiEnhanced Lab of Ferrometallurgy; Shanghai 200072). HIGH ORDER SUB-REGULAR SOLUTION MODEL AND ITS APPLICATIONS IN THE CALCULATION OF COMPONENT ACTIVITIES OF MnO-SiO_2-Al_2O_3-CaO MOLTEN SLAG[J]. 金属学报, 1997, 33(10): 1085-1093.
No Suggested Reading articles found!