| THERMODYNAMICS OF TERNARY Fe-B-Si MELTS AT 1450℃ Ⅰ. ACTIVITY OF Si AND ITS INTERACTION COEFFICIENTS |
| JI Chunlin;YU Rongxiang;LIU Sulan Northeast University of Technology; ShenyangLIU Sulan Lecturer;Department of Metallurgleal Phusicat Chemistry;Northeoss University of Technology;Shenyang |
|
Cite this article:
JI Chunlin;YU Rongxiang;LIU Sulan Northeast University of Technology; ShenyangLIU Sulan Lecturer;Department of Metallurgleal Phusicat Chemistry;Northeoss University of Technology;Shenyang. THERMODYNAMICS OF TERNARY Fe-B-Si MELTS AT 1450℃ Ⅰ. ACTIVITY OF Si AND ITS INTERACTION COEFFICIENTS. Acta Metall Sin, 1988, 24(2): 155-160.
|
|
|
Abstract Iso-activity lines of Si in ternary Fe-B-Si melts were measured at1450℃ with Ag-bath medium method. The activity of Si in Ag-Si alloy was alsodetermined by means of the EMF measurement of a Si-concentration cell in whicha double-tubed ZrO_2 electrolyte was used. A method has been proposed for calculat-ing ln γ°_(Si) and the first and second order interaction coefficients from the experi-mental data; Following results have been obtained: ln γ°_(Si)=-3.19, ε_(Si)~(Si)=7.0, ρ_(Si)~(Si)=6.5, ε_(Si)~B=16.0, ρ_(Si)~B=-12.0 and ρ_(Si)~(Si,B)=40.8
|
|
Received: 18 February 1988
|
1 Wagner C. Thermodynamic of,Alloys, Reading Mass: Addison-Wesley. 1952: 51 2 Lupis C H P, Elliott J F. Acta Metall. 1966; 14: 529. 1019 3 Elliott J F, Gleiser M, Ramakrishna V. Thermochemistry for Steelmaking II, Reading Mass: Addison-Wesley, 1963: 4 Schenck H, Steinmetz E. Arch Eisenhuettenwes, 1968; 39: 255 5 松下幸雄,坂尾弘,大谷正康等,制钢反应推奖平衡值,日本学术振兴会,1968: 6 Sigworth G K,Elliott J F.Met Sci,1974;8:298 7 松下幸雄,坂尾弘,大谷正康等,制钢反应推奖平衡值,(改订增补)日本学术振兴会,1984: 8 Ball D L. Trans Metall Soc AIME, 1967; 239: 31 9 Schroeder D, Chipman J. Trans Metall Soc AIME, 1964; 230: 1492. 10 #120 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|