INFLUENCE OF MOULD ROTATION ON MACROSEGREGATION IN INGOT |
YU Qiuping;ZHOU Yaohe Northwestern Polytechnical University; Xi'an |
|
Cite this article:
YU Qiuping;ZHOU Yaohe Northwestern Polytechnical University; Xi'an. INFLUENCE OF MOULD ROTATION ON MACROSEGREGATION IN INGOT. Acta Metall Sin, 1988, 24(5): 379-384.
|
Abstract The macrosegregation formation in an ingot and the influence of rotat-ing mould upon it were analysed on the basis of the interdendritic flow. When theingot mould rotates unidirectionally, the centrifugal volume force acts on all innerparts and when the ingot mould rotates attenately, the tangential alternate force isalso formed, and both have various influences on the different modes of interden-dritic flow. It is shown that as the ingot mould rotates unidirectionally or alterna-tely with moderate angular speed, the interdendritic unstable flow may be control-led effectively and the formation of segregation may be restrained. Thus, it seemsto be significant for reducing the segregation such as A-type, etc., in the steel in-got.
|
Received: 18 May 1988
|
1 Kirkaldy J S, Youdelis W V. Trans Metall Soc AIME, 1958; 212: 833--840 2 Mehrabian R, Keane M, Flemings M C. Metall Trans, 1970; 1: 1209--1220 3 McDonald R J. Hunt J D. Trans Metall Soc AIME, 1969; 245: 1993--1997 4 Stewart M J, MacAulay L C. Weinberg P. Metall Trans, 1971; 2: 169--173 5 Kou S, Poirier D R Flemings M C. Metall Trans 1978; 9B: 711--719 6 Moore J J, Shah N A. Int Metall Rev, 1983; 28: 338--356 7 喻秋平,枝晶间液相流动与宏观偏析,西北工业大学科技资料,CL8613,1986 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|