| IN SITU OBSERVATION AND MECHANISM STUDY OF FORMATION OF BASKET DURING BAINITIC TRANSFORMATION |
| WANG Yingshu;SUN Fuyu;XU Wenchong Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing |
|
Cite this article:
WANG Yingshu;SUN Fuyu;XU Wenchong Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing. IN SITU OBSERVATION AND MECHANISM STUDY OF FORMATION OF BASKET DURING BAINITIC TRANSFORMATION. Acta Metall Sin, 1989, 25(1): 68-70.
|
|
|
Abstract By means of HM-100 hot-stage microscopy, the in situ observation of γ→β trans-formation in steel 12Cr2MoWVTiB has been carried out The sequence of the growth of ferriticneedles composing bainitic basket has also been determined. A multislip system transform modelconcerning the formation of basket has been proposed.
|
|
Received: 18 January 1989
|
1 Ko T (柯俊), Cottrell S A. J Iron Steel Inst, 1952; 172: 307 2 Hillert M. Metall Trans, A, 1985; 16: 13 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|