| THERMAL HYDROGEN EVOLUTION TECHNIQUE STUDY OF TRAPPED HYDROGEN IN 18NI MARAGING STEEL |
| YAO Daping;CHEN Wenxiu Institute of Metal Research; Academia Sinica; Shenyang |
|
Cite this article:
YAO Daping;CHEN Wenxiu Institute of Metal Research; Academia Sinica; Shenyang. THERMAL HYDROGEN EVOLUTION TECHNIQUE STUDY OF TRAPPED HYDROGEN IN 18NI MARAGING STEEL. Acta Metall Sin, 1989, 25(1): 71-74.
|
|
|
Abstract The inieraction of hydrogen with intetface between the precipitates and the martens-itic matrix in 18Ni maraging steel has been studied by means of thermal hydrogen evolutiontechnigue using gas chromatograph as hydrogen detector. An evolution rate peak has been obser-ved at 451K. The hight of the peak relates to the amount and distribution of the precipitates.The activation energy needed to escape the hydrogen from the trap sites is 23.2 kJ/mol.
|
|
Received: 18 January 1989
|
1 Andrew J H, Lee H (李薰), Quarrell A G. J Iron Steel Inst, 1942; 146 (2) : 181 2 Choo W Y, Lee J Y. Metall Trans, 1983; 14A: 1299 3 Choo W Y, Lee J Y. Metall Trans, 1982; 13A: 135 4 Lee H G, Lee J Y. Acta Metall, 1984; 32: 131 5 姚大平,中国科学院金属研究所硕士论文,1987 6 Oriani R A.Acta Metall, 1970; 18: 147 7 朱静,李荣,张丽萍,金属学报,1986;22:A304 8 坂本芳一,长谷一德.日本金属学会志,1979;43;190 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|