INFLUENCE OF SOME FACTORS ON FLUID FLOW IN CONTINUOUS CASTING TUNDISHES
HE Youduo;Y. SAHAI Baotou Institute of Iron & Steel Technology The Ohio State University
Cite this article: 

HE Youduo;Y. SAHAI Baotou Institute of Iron & Steel Technology The Ohio State University. INFLUENCE OF SOME FACTORS ON FLUID FLOW IN CONTINUOUS CASTING TUNDISHES. Acta Metall Sin, 1989, 25(4): 132-136.

Download:  PDF(447KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  This paper, in which the influence of some factors on velocity fieldin continuous casting tundishes has been verified by means of computer simulation,is the extension of the paper "Fluid dynamics of continuous casting tundishes.These factors are tundish wall inclination; the dimensionless geometric size of tun-dish; the double-angle tundish; the dimension and location of weir and dam. Someuseful conclusions may be extracted finally for practice and design from this paper.
Key words:  continuous casting tundish      flow field     
Received:  18 April 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I4/132

1 贺友多,Sahai Y.金属学报,1988;24:B79--86
2 Launder B E, Spalding D B. Comput Method Appl Mech Eng, 1974; 3: 269
3 Launder B E, Spalding D B. Heat Transfer Section Report, No. HTS/73/2, Imperial College, London, 1973
4 王应时,范维澄,周力行,徐旭常.燃烧过程数值计算,北京:科学出版社,1986
5 窦国仁.紊流力学,北京:人民教育出版社,1984
6 陈景仁.流体力学及传热学,北京:国防工业出版社,1984
7 Hinze J O. Turbulence, New York: McGraw-Hill, 1959
8 Gosman A D, Launder B E. TEACH-2E, Internal Report, Mech Eng Dept, Imperial College, London, 1976
9 He Y, Sahai Y. Metal Trans, 1987; 18B: 81--92
10 Patanker S V. Numerical Heat Transfer and Fluid Flow, New York: McGraw-Hill, 1980
11 Sahai Y, Guthrie R I L. Metal Trans, 1982; 13B: 193--202
12 Sahai Y, Guthrie R I L. Metal Trans, 1982; 13B: 203--210
[1] TANG Haiyan, LIU Jinwen, WANG Kaimin, XIAO Hong, LI Aiwu, ZHANG Jiaquan. Progress and Perspective of Functioned Continuous Casting Tundish Through Heating and Temperature Control[J]. 金属学报, 2021, 57(10): 1229-1245.
[2] WANG Fuqiang, LIU Wei, WANG Zhaowen. Effect of Local Cathode Current Increasing on Bath-Metal Two-Phase Flow Field in Aluminum Reduction Cells[J]. 金属学报, 2020, 56(7): 1047-1056.
[3] TANG Haiyan, LI Xiaosong, ZHANG Shuo, ZHANG Jiaquan. Fluid Flow and Heat Transfer in a Tundish with Channel Induction Heating for Sequence Casting with a Constant Superheat Control[J]. 金属学报, 2020, 56(12): 1629-1642.
[4] Chenglin LIU, Haijun SU, Jun ZHANG, Taiwen HUANG, Lin LIU, Hengzhi FU. Effect of Electromagnetic Field on Microstructure ofNi-Based Single Crystal Superalloys[J]. 金属学报, 2018, 54(10): 1428-1434.
[5] Linyuan HAN, Xuan LI, Chenglin CHU, Jing BAI, Feng XUE. Corrosion Behavior of AZ31 Magnesium Alloy in Dynamic Conditions[J]. 金属学报, 2017, 53(10): 1347-1356.
[6] Bin XU,Qingxian HU,Shujun CHEN,Fan JIANG,Xiaoli WANG. NUMERICAL SIMULATION OF DYNAMIC BEHAVIOR OF KEYHOLE AND MOLTEN POOL AT K-PAW QUASI STEADY PROCESS[J]. 金属学报, 2016, 52(7): 804-810.
[7] LI Baokuan DAI Fengyu QI Fengsheng YANG Ran. FLOW FIELD AND CONCENTRATION FIELD OF ALLOYING ADDITION IN CLAD STEEL CONTINUOUS CASTING MOLD USING LONG AND SHORT NOZZLES[J]. 金属学报, 2010, 46(6): 736-742.
[8] YU Haiqi ZHU Miaoyong. 3-D NUMERICAL SIMULATION OF FLOW FIELD AND TEMPERATURE FIELD IN A ROUND BILLET CONTINUOUS CASTING MOLD WITH ELECTROMAGNETIC STIRRING[J]. 金属学报, 2008, 44(12): 1465-1473.
[9] Miao-Yong ZHU. WATER MODEL STUDY ON MECHANISM OF INCLUSION REMOVAL IN CONTINUOUS CASTING TUNDISH[J]. 金属学报, 2007, 43(9): 1004-1008 .
[10] ZHU Miaoyong(Northeastern Universily; Shenyang 110006). NUMERICAL SIMULATION OF THE COUPLED MOLTEN STEEL FLOW AND HEAT TRANSFER IN CONTINUOUS CASTING TUNDISHES[J]. 金属学报, 1997, 33(9): 933-938.
[11] LI Baokuan;HE Jicheng;JIA Guanglin;GAO Yunyan(Northeastern University; Shenyang 110006). ELECTROMAGNETIC BRAKING ON FLOW FIELD OF MOLTEN STEEL IN THE THIN-SLAB CONTINUOUS CASTING MOLD[J]. 金属学报, 1997, 33(11): 1207-1214.
[12] ZHU Miaoyong(Northeastern University;Shenyang 110006);SAW ADA Ikuo (Nippon Steel Corporation; Kawasaki 211;Japan). NUMERICAL SIMULATION OF THREE-DIMENSIONAL TURBULENT FLOW IN CONTINUOUS CASTING TUNDISHES[J]. 金属学报, 1997, 33(11): 1215-1221.
[13] SHENG Dongyuan; NI Mansen; DENG Kaiwen; LIU Jiaqi; GAN Yong; XIAO Zeqiang (National Research & Engineering Center of Continuous Casting Technology;Gentral Iron and Steel Research Institute; Ministry of Metallurgical industry;Beijing 100081)(Manuscript received 1995-11-09; in revised form 1996-04-17). MATHEMATICAL MODEL OF FLUID FLOW,TEMPERATURE CONTROL AND INCLUSION BEHAVIOUR IN CONTINUOUS CASTING TUNDISH[J]. 金属学报, 1996, 32(7): 742-748.
[14] WEI Jihe(WEI Chiho)(Shanghai University);REN Yongli(Xi'an Institute of Metallurgy and Construction Engineering)(Manuscript received 19 February; 1994). MATHEMATICAL MODELLING OF SLAG FLOW FIELD IN ESR SYSTEM[J]. 金属学报, 1994, 30(23): 481-490.
[15] QU Ying;YANG Jian;XU Baomei University of Science and Technology Beijing Department of Metallurgy;University of Science and Technology Beijing; Beijing 100083. MATHEMATICAL MODELLING OF FLOW PHENOMENA IN METAL BATH COVERED WITH MOLTEN SLAG[J]. 金属学报, 1990, 26(3): 85-91.
No Suggested Reading articles found!