| INFLUENCE OF SOME FACTORS ON FLUID FLOW IN CONTINUOUS CASTING TUNDISHES |
| HE Youduo;Y. SAHAI Baotou Institute of Iron & Steel Technology The Ohio State University |
|
Cite this article:
HE Youduo;Y. SAHAI Baotou Institute of Iron & Steel Technology The Ohio State University. INFLUENCE OF SOME FACTORS ON FLUID FLOW IN CONTINUOUS CASTING TUNDISHES. Acta Metall Sin, 1989, 25(4): 132-136.
|
|
|
Abstract This paper, in which the influence of some factors on velocity fieldin continuous casting tundishes has been verified by means of computer simulation,is the extension of the paper "Fluid dynamics of continuous casting tundishes.These factors are tundish wall inclination; the dimensionless geometric size of tun-dish; the double-angle tundish; the dimension and location of weir and dam. Someuseful conclusions may be extracted finally for practice and design from this paper.
|
|
Received: 18 April 1989
|
1 贺友多,Sahai Y.金属学报,1988;24:B79--86 2 Launder B E, Spalding D B. Comput Method Appl Mech Eng, 1974; 3: 269 3 Launder B E, Spalding D B. Heat Transfer Section Report, No. HTS/73/2, Imperial College, London, 1973 4 王应时,范维澄,周力行,徐旭常.燃烧过程数值计算,北京:科学出版社,1986 5 窦国仁.紊流力学,北京:人民教育出版社,1984 6 陈景仁.流体力学及传热学,北京:国防工业出版社,1984 7 Hinze J O. Turbulence, New York: McGraw-Hill, 1959 8 Gosman A D, Launder B E. TEACH-2E, Internal Report, Mech Eng Dept, Imperial College, London, 1976 9 He Y, Sahai Y. Metal Trans, 1987; 18B: 81--92 10 Patanker S V. Numerical Heat Transfer and Fluid Flow, New York: McGraw-Hill, 1980 11 Sahai Y, Guthrie R I L. Metal Trans, 1982; 13B: 193--202 12 Sahai Y, Guthrie R I L. Metal Trans, 1982; 13B: 203--210 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|