Please wait a minute...
Acta Metall Sin  1989, Vol. 25 Issue (4): 148-150    DOI:
Current Issue | Archive | Adv Search |
OBSERVATION ON SPUTTERING SURFACE OF ALLOYS IN GLOW DISCHARGE
REN Jianshi;ZHAO Huilin;ZHANG Gongshu Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

REN Jianshi;ZHAO Huilin;ZHANG Gongshu Institute of Metal Research; Academia Sinica; Shenyang. OBSERVATION ON SPUTTERING SURFACE OF ALLOYS IN GLOW DISCHARGE. Acta Metall Sin, 1989, 25(4): 148-150.

Download:  PDF(1308KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Glow discharge cathodic sputtering of alloys containing second phase precipitatesor injection of oxide particles has been observed with an energy dispersive X-ray spectrometerand scanning electron microprobe. It was shown that the formation of cones during thesputtering in these alloys is due to masking of the matrix by glow sputtering second phaseprecipitates or oxide particles. At steady state, the number density was lound to be a functionof precipitate or oxide particle density in bulk alloys. In addition to local sputtering rate changes,the electrostate effect ?ay play a role in the formation of cones.
Key words:  glow discharge      cathodic sputtering      nickel base alloy     
Received:  18 April 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I4/148

1 Jager H, Blum F. Spectrochim Acta, 1974; 29B: 73
2 Greene J E, Natarajan B R. J Appl Phys, 1978; 49: 417
3 张匀,赵洪恩,郭建亭.金属学报,1988;24:A63
4 张洪度,于波,任建世.分析化学,1980;8:265B
[1] HUA Hanyu,XIE Jun,SHU Delong,HOU Guichen,Naicheng SHENG,YU Jinjiang,CUI Chuanyong,SUN Xiaofeng,ZHOU Yizhou. Influence of W Content on the Microstructure of Nickel Base Superalloy with High W Content[J]. 金属学报, 2020, 56(2): 161-170.
[2] Meiqiong OU,Yang LIU,Xiangdong ZHA,Yingche MA,Leming CHENG,Kui LIU. CORROSION BEHAVIOR OF A NEW NICKEL BASE ALLOY IN SUPERCRITICAL WATERCONTAINING DIVERSE IONS[J]. 金属学报, 2016, 52(12): 1557-1564.
[3] REN Jianshi;ZHANG Gongshu;WANG Zhenshu;LIU Gen;LIU Shenglin Institute of Metal Research; Academia Sinica; Shenyang; Shanghai University of Technology Correspondent senior engineer; Institute of Metal Research; Academia Sinica; Shenyang 110015. CORRELATION BETWEEN CONSTITUENT AND SPUTTERING RATE OF BINARY ALLOYS IN GLOW DISCHARGE LAMP[J]. 金属学报, 1992, 28(5): 85-89.