EVALUATION OF PERMEABILITY STABILITY OF SEVERAL AMORPHOUS FERROMAGNETIC ALLOYS |
ZHANG Yanzhong Shanghai Iron and Steel Research Institute ZHANG Yanzhong. senior engineer;Steel Research Institute; Shanghai Measuring and Testing Centre; Shanghai Iron and 200990 |
|
Cite this article:
ZHANG Yanzhong Shanghai Iron and Steel Research Institute ZHANG Yanzhong. senior engineer;Steel Research Institute; Shanghai Measuring and Testing Centre; Shanghai Iron and 200990. EVALUATION OF PERMEABILITY STABILITY OF SEVERAL AMORPHOUS FERROMAGNETIC ALLOYS. Acta Metall Sin, 1989, 25(6): 116-119.
|
Abstract The evaluation of the relative stability of initial permeability hasbeen made for the pre-annealed amorphous ferromagnetic alloys Fe_(76)Si_(10)B_(14), Fe_(40)Ni_(38)Mo_4B_(18) and (Fe_(0.1)Ni_(0.35)Co_(0.55))_(78)Si_8B_(14) by the experlmental values of average activa-tion energy and frequency factors on the basis of the empirical expression deducedby experimental data of the kinetics of their permeability decay. Calculated resultsshow that the relative stability of permeability is sufficient for practical uses inthe temperature range within 100℃, although the permeability instability can notbe substantially eliminated. In other words, the permeability decay is considerablysmall within a period of considerable length.
|
Received: 18 June 1989
|
1 张延忠.金属学报,1985;21:B189 2 Zhang Y Z (张延忠). KEXUE TONGBAO (科学通报), 1986; 3l: 747 3 Zhang Yanzhong (张延忠), Miao Jianxin (苗建新). J Phys F, 1987; 17: 767 4 Zhang Yanzbong (张延忠). Phys Stat Sol, (a), 1988; 106: 207 5 Hesse J, Ruebartsch A, J Phys E. 1974; 7: 526 |
No Suggested Reading articles found! |
|
|