EVALUATION OF PERMEABILITY STABILITY OF SEVERAL AMORPHOUS FERROMAGNETIC ALLOYS
ZHANG Yanzhong Shanghai Iron and Steel Research Institute ZHANG Yanzhong. senior engineer;Steel Research Institute; Shanghai Measuring and Testing Centre; Shanghai Iron and 200990
Cite this article: 

ZHANG Yanzhong Shanghai Iron and Steel Research Institute ZHANG Yanzhong. senior engineer;Steel Research Institute; Shanghai Measuring and Testing Centre; Shanghai Iron and 200990. EVALUATION OF PERMEABILITY STABILITY OF SEVERAL AMORPHOUS FERROMAGNETIC ALLOYS. Acta Metall Sin, 1989, 25(6): 116-119.

Download:  PDF(357KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The evaluation of the relative stability of initial permeability hasbeen made for the pre-annealed amorphous ferromagnetic alloys Fe_(76)Si_(10)B_(14), Fe_(40)Ni_(38)Mo_4B_(18) and (Fe_(0.1)Ni_(0.35)Co_(0.55))_(78)Si_8B_(14) by the experlmental values of average activa-tion energy and frequency factors on the basis of the empirical expression deducedby experimental data of the kinetics of their permeability decay. Calculated resultsshow that the relative stability of permeability is sufficient for practical uses inthe temperature range within 100℃, although the permeability instability can notbe substantially eliminated. In other words, the permeability decay is considerablysmall within a period of considerable length.
Key words:  permeability decay      activation energy      frequency factor     
Received:  18 June 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I6/116

1 张延忠.金属学报,1985;21:B189
2 Zhang Y Z (张延忠). KEXUE TONGBAO (科学通报), 1986; 3l: 747
3 Zhang Yanzhong (张延忠), Miao Jianxin (苗建新). J Phys F, 1987; 17: 767
4 Zhang Yanzbong (张延忠). Phys Stat Sol, (a), 1988; 106: 207
5 Hesse J, Ruebartsch A, J Phys E. 1974; 7: 526
[1] Shubo LI, Wenbo DU, Xudong WANG, Ke LIU, Zhaohui WANG. Effect of Zr Addition on the Grain Refinement Mechanism of Mg-Gd-Er Alloys[J]. 金属学报, 2018, 54(6): 911-917.
[2] HU Ke, LI Xiaoqiang, QU Shengguan, YANG Chao, LI Yuanyuan. DEVELOPMENT OF MASTER SINTERING CURVE FOR SPARK PLASMA SINTERING OF 93W-5.6Ni-1.4Fe HEAVY ALLOY[J]. 金属学报, 2014, 50(6): 727-736.
[3] ZHOU Xiaowei SHEN Yifu GU Dongdong. MICROSTRUCTURE AND HIGH TEMPERATURE OXIDATION RESISTANCE OF NANOCRYSTALLINE Ni–CeO2 COMPOSITE COATINGS DEPOSITED BY DOUBLE–PULSED ELECTRO DEPOSITION[J]. 金属学报, 2012, 48(8): 957-964.
[4] ZHU Hongyan, MA Weimin, WEN Lei, GUAN Renguo,MA Lei, WU Nan. SYNTHESIS KINETICS OF (Y, Gd)2O3∶Eu3+ NANO-POWDERS DURING PROCESS OF PREPARATION[J]. 金属学报, 2012, 48(6): 671-677.
[5] TIAN Chenggang CUI Chuanyong GU Yuefeng SUN Xiaofeng . EFFECT OF SOLUTION TREATMENT ON THE INVERSE DYNAMIC STRAIN AGING OF A Ni–Co BASE SUPERALLOY[J]. 金属学报, 2012, 48(10): 1223-1228.
[6] SONG Renbo ZHANG Yongkun WEN Xinli JIA Yisu. HOT DEFORMATION BEHAVIOR OF A HIGH STRENGTH CONTAINER STEEL COMPOUNDED WITH Nb-B[J]. 金属学报, 2011, 47(1): 34-40.
[7] CHEN Liqing ZHAO Yang XU Xiangqiu LIU Xianghua. DYNAMIC RECRYSTALLIZATION AND PRECIPITATION BEHAVIORS OF A KIND OF LOW CARBON V–MICROALLYED STEEL[J]. 金属学报, 2010, 46(10): 1215-1222.
[8] HAN Lizhan CHEN Ruikai GU Jianfeng PAN Jiansheng. BEHAVIOR OF AUSTENITE GRAIN GROWTH IN X12CrMoWVNbN10-1-1 FERRITE HEAT-RESISTANT STEEL[J]. 金属学报, 2009, 45(12): 1446-1450.
[9] KANG Mokuang ZHANG Mingxing LIU Feng ZHU Ming. OVERALL ACTIVATION ENERGY OF ISOTHERMAL TRANSFORMATION IN METAL ALLOY AND ITS MECHANISM II. Isothermal Transformation in β Brasses[J]. 金属学报, 2009, 45(1): 32-36.
[10] XU Min YI Jun QUAN Mingxiu WANG Yandong ZUO Liang. EFFECT OF Nb ON CRYSTALLIZATION KINETICS OF Fe-Co-Nd-B AMORPHOUS ALLOYS[J]. 金属学报, 2009, 45(1): 91-96.
[11] KANG Mokuang ZHANG Mingxing LIU Feng ZHU Ming. OVERALL ACTIVATION ENERGY OF ISOTHERMAL TRANSFORMATION IN METAL ALLOY AND ITS MECHANISM I. Medium Temperature (Bainite) Isothermal Transformation in Steels[J]. 金属学报, 2009, 45(1): 25-31.
[12] . XRD Investigation of The Recrystallization Process of Shot Peened Layer on In-Situ TiB2/6351Al[J]. 金属学报, 2008, 44(6): 671-674 .
[13] LIU Jiangtao;WANG Zhongguang;SHANG Jianku. DEFORMATION BEHAVIORS OF [110] AND [112] ORIENTED β-Sn SINGLE CRYSTALS[J]. 金属学报, 2008, 44(12): 1409-1414.
[14] . Constitutive Relationship of Hot Deformation of AZ91 Magnesium Alloy[J]. 金属学报, 2008, 44(11): 1378-1383 .
[15] LI Jiguang;SUN Xudong;WANG Yarong;DONG Wenxin;RU Hongqiang;HAO Shiming (School of Materials and Metallurgy; Northeastern University; Shenyang 110006). STUDY OF INITIAL STAGE SINTERING OF NANOCRYSTALLINE α-Al_2O_3 POWDER BY ISOTHERMAL METHOD[J]. 金属学报, 1998, 34(2): 189-194.
No Suggested Reading articles found!