| A CONTINUOUS DAMAGE APPROACH TO RELATIONSHIP BETWEEN SIZE REDUCTION AND ENERGY CONSUMPTION DURING ORE COMMINUTION |
| ZHU Yi;XU Xiaohe Northeast University of Technology; Shenyang Department of Mining;Northeast University of Technology;Shenyang 110006 |
|
Cite this article:
ZHU Yi;XU Xiaohe Northeast University of Technology; Shenyang Department of Mining;Northeast University of Technology;Shenyang 110006. A CONTINUOUS DAMAGE APPROACH TO RELATIONSHIP BETWEEN SIZE REDUCTION AND ENERGY CONSUMPTION DURING ORE COMMINUTION. Acta Metall Sin, 1990, 26(3): 81-84.
|
|
|
Abstract Based upon the aspect of continuous damaging, the process of ore com-minution may be described as the growth and propagation of the microcraks in theore grains under external loading, and a theoretical expression has been developed onthe relationship between the grain size distribution and the total energy consumptionduring entire ore comminution process. The energy consumed totally may be consi-dered to consist of two portions: i.e., with fresh crack surfaces growth and withcrack propagation. The expression proposed seems to be an advance over previousconventional ones, especially that from the viewpoint of energy distribution.
|
|
Received: 18 March 1990
|
1 Zhu Yi, Xu Xiao-he. J Eng Fract Mech, 1990; 35: 647 2 Kachanov L M. Mech Mater, 1982; 1: 19 3 朱毅,徐小荷.有色金属,1989;41:1 4 Perry J H. Chemical Engineer Handbook, 3rd ed., New York: McGraw-Hill, 1950: 417 5 朱毅.东北工学院博士论文,1988 6 Schuhmann R J. AIME TP 1189, 1940 7 Charles R J. Trans AIME, 1957; 208: 80 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|