A CONTINUOUS DAMAGE APPROACH TO RELATIONSHIP BETWEEN SIZE REDUCTION AND ENERGY CONSUMPTION DURING ORE COMMINUTION
ZHU Yi;XU Xiaohe Northeast University of Technology; Shenyang Department of Mining;Northeast University of Technology;Shenyang 110006
Cite this article: 

ZHU Yi;XU Xiaohe Northeast University of Technology; Shenyang Department of Mining;Northeast University of Technology;Shenyang 110006. A CONTINUOUS DAMAGE APPROACH TO RELATIONSHIP BETWEEN SIZE REDUCTION AND ENERGY CONSUMPTION DURING ORE COMMINUTION. Acta Metall Sin, 1990, 26(3): 81-84.

Download:  PDF(375KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based upon the aspect of continuous damaging, the process of ore com-minution may be described as the growth and propagation of the microcraks in theore grains under external loading, and a theoretical expression has been developed onthe relationship between the grain size distribution and the total energy consumptionduring entire ore comminution process. The energy consumed totally may be consi-dered to consist of two portions: i.e., with fresh crack surfaces growth and withcrack propagation. The expression proposed seems to be an advance over previousconventional ones, especially that from the viewpoint of energy distribution.
Key words:  ore comminution      continuous damage      critical perfectness      damage factor     
Received:  18 March 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I3/81

1 Zhu Yi, Xu Xiao-he. J Eng Fract Mech, 1990; 35: 647
2 Kachanov L M. Mech Mater, 1982; 1: 19
3 朱毅,徐小荷.有色金属,1989;41:1
4 Perry J H. Chemical Engineer Handbook, 3rd ed., New York: McGraw-Hill, 1950: 417
5 朱毅.东北工学院博士论文,1988
6 Schuhmann R J. AIME TP 1189, 1940
7 Charles R J. Trans AIME, 1957; 208: 80
[1] ZHENG Junzi, ZHANG Laiqi, HOU Yongming, MA Xiangling, LIN Junpin. QUASI ISOTHERMAL FORGING SIMULATION OF β-γ TiAl ALLOY CONTAINING HIGH CONTENT OF Nb[J]. 金属学报, 2013, 49(11): 1439-1444.
No Suggested Reading articles found!