| INFLUENCE OF GRAIN SHAPE AND CARBIDE ON CREEP CRACK GROWTH IN HK40 |
| ZHU Shijie;ZHAO Jie;WANG Fugang Institute of Metal Research; Academia Sinica; Shenyang Fushun Institute of Petrochemistry Dalian University of Technology |
|
Cite this article:
ZHU Shijie;ZHAO Jie;WANG Fugang Institute of Metal Research; Academia Sinica; Shenyang Fushun Institute of Petrochemistry Dalian University of Technology. INFLUENCE OF GRAIN SHAPE AND CARBIDE ON CREEP CRACK GROWTH IN HK40. Acta Metall Sin, 1990, 26(3): 77-80.
|
|
|
Abstract The influence of two different grain shapes and carbides in the HK40 alloy,the material for use of furnace tube, on the rate of creep crack growth has been investigated.The material of columnar grain is inferior resistance against creep crack growth to that ofequiaxial grain, when the load line is perpendicular to the columnar grain axis. The influenceof secondary carbides on the rate of creep crack propagation is dependent upon the grain shape.
|
|
Received: 18 March 1990
|
1 曹智本,陆善炘,程蓉娟.大连工学院学报,1981;20(3) :1 2 李德俊,曹智本.物理测试,1986;(6) :1 3 Zhu S J, Li P E, Zhao J, Cao Z B. Mater Sci Eng 1989; A114: 7 4 Nazmy M Y. Scr Metall, 1983; 17: 491 5 Zhu S J, Zhu S M, Wang F G. Scr Metall, 1989; 23: 1845 6 朱世杰.大连理工大学博士论文,1989 7 Floreen S. Metall Trans, 1975; 6A: 1741 8 Dunlop G L, Twigg R J, Taplin D M R. Scand J Metall, 1978; 7: 15 |