| SUPERPLASTIC DEFORMATION BEHAVIOUR OF SUPERHARD Al ALLOY LC4 |
| JIANG Xinggang;WU Qingling;CUI Jianzhong;MA Longxiang Northeast University of Technology; Shenyang Department of Metal Working; Northeast University of Technclogy;Shenyang 110006 |
|
Cite this article:
JIANG Xinggang;WU Qingling;CUI Jianzhong;MA Longxiang Northeast University of Technology; Shenyang Department of Metal Working; Northeast University of Technclogy;Shenyang 110006. SUPERPLASTIC DEFORMATION BEHAVIOUR OF SUPERHARD Al ALLOY LC4. Acta Metall Sin, 1990, 26(4): 158-160.
|
|
|
Abstract The superplasticity of the high strength and hard Al alloy LC4 was improved toa great extent by modified thermomechanic treatment. Its maximum elongation may be up to2100% under deformation with initial strain rate 8.33×10~(-4)s~(-1) at 510℃. The optical and TEMobservations of the microstructure changes revealed that with thein crease of deformation, the dis-location density increases, the grain grows and the alloy exhibits strain hardening. The excel-lent elongation of the alloy seems due to the increase of grain stability under deformation.
|
|
Received: 18 April 1990
|
1 Hamilton C H, Bampton C C, Paton N E. In: Paton N E, Hamilton C H eds., Superplastic Forming of Structural Alloys, AIME, 1982: 173 2 周善佑,汪立勤.上海交通大学学报,1985;19:70 3 周善佑,汪立勤.上海交通大学学报,1989;23:24 4 Wert J A, Paton N E, Hamilton C H, Mahoney M W. Metall Trans, 1981; 12A: 1267 5 Wert J A. Ser Metall, 1981; 15: 445 6 蒋兴钢,东北工学院硕士论文,1987C |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|