| EFFECT OF MICROSTRUCTURE ON CORROSIONFATIGUE BEHAVIOUR OF LOWCARBON BAINITE STEEL |
| ZHANG Rong;ZHOU Lubin Northwestern Polytechnical University; Xi'an; ZHENG Wenlong; HUA Huizhong Shanghai Research Institute of Materials |
|
Cite this article:
ZHANG Rong;ZHOU Lubin Northwestern Polytechnical University; Xi'an; ZHENG Wenlong; HUA Huizhong Shanghai Research Institute of Materials. EFFECT OF MICROSTRUCTURE ON CORROSIONFATIGUE BEHAVIOUR OF LOWCARBON BAINITE STEEL. Acta Metall Sin, 1991, 27(4): 116-120.
|
|
|
Abstract The behaviour towards corrosion fatigue of low carbon bainite steelwith various microstructures after tempered at different temperatures has been exa-mined. The susceptibility of the steel to corrosion fatigue may be improved by tem-pering at 300℃:
|
|
Received: 18 April 1991
|
1 张蓉.西北工业大学硕士学位论文.1988 2 Kerr R, Solana F, Bernstein I M, Thompson A W. Metall Trans, 1987; 18A: 1011 3 高惠临,谈育煦,王笑天.金属学报,1988;24:A17 4 Solana F, Takamadate C, Bernstein I M. Thompson A W. Metall Trans. 1987; 18A: 1023 5 彦连治,王清华,崔文宣.第一届全国贝氏体相变会议论文集,中国金属学会材料科学学会,广东惠州,1987:18 6 胡光立.第一届全国贝氏体相变会议论文集,中国金属学会材料科学学会,广东惠州,1987:115 |