SYMMETRICAL SUPERLATTICE INTRINSJC STACKING FAULTS IN DEFORMEDPOLYCRYSTALLINE Ni_3 Al AND THEIR FORMATION MECHANISM |
YAN Wen Xi'an Institute of Technology Correspondent associate professor;xi'an Institute of Technology |
|
Cite this article:
YAN Wen Xi'an Institute of Technology Correspondent associate professor;xi'an Institute of Technology. SYMMETRICAL SUPERLATTICE INTRINSJC STACKING FAULTS IN DEFORMEDPOLYCRYSTALLINE Ni_3 Al AND THEIR FORMATION MECHANISM. Acta Metall Sin, 1991, 27(5): 8-13.
|
Abstract TEM analysis and computer simulation of the symmetrical superlattice intrinsic stacking faults (SISFs) in slightly deformed polycrystalline Ni_3Al at room temperature are presented. The symmetrical SISFs are important components of the crystal defects in deformed Ni_3Al alloys; the formation mechanism of the symmetrical SISF can be resulted from the reorientation, dissociation and annihilation of a dipole on {111} plane under applied shear stress.
|
Received: 18 May 1991
|
1 Takeuchi S, Kuramoto E, Yamamoto T, Taoka T. Jpn J Appl phys, 1973; 12: 1486--1592 2 Baker I, Schulson E M. Phys Status Solidi, 1984; A85: 481--490 3 Baker I, Schulson E M. Phys Status Solidi, 1985; A89: 163--172 4 Baker I, Schulson E M, Horton J A. Acta Metall, 1987; 35: 1533--1541 5 Yan W, Jones I P, Smallman R E. Ser Metall, 1987; 21: 1511--1515 6 严文.兵器材料科学与工程,1989;8:103--111 7 Pak H-R, Saburi T, Nenno S. Ser Metall, 1976; 10: 1081--1085 8 Pope D P, Ezz S S. Int Met Rev, 1984; 29: 136--167 9 Yan W PhD Dissertation, University of Birmingham, UK, 1988 10 Head A K, Humble P, Clarebrough L M, Morton A J, Forwood C T. Computed Electron Micrographs and Defect Identification, Amsterdam: North-Holland, 1973 11 Suzuki K, Kuramoto E, Takeuchi S, Ichihara M. Jpn J Appl Phys, 1977; 16: 919--923 12 Suzuki K, Ichihara M, Takeuchi S. Acta Metall, 1979; 27: 193--200 |