PREPARATION OF ULTRAFINE ALLOY POWDER BY REDUCTION OF COMPLEX OXIDE
QIAN Yitai;FU Peizhen;CAO Guanghan;CHEN Zuyao University of Science and Technology of China; Hefei
Cite this article: 

QIAN Yitai;FU Peizhen;CAO Guanghan;CHEN Zuyao University of Science and Technology of China; Hefei. PREPARATION OF ULTRAFINE ALLOY POWDER BY REDUCTION OF COMPLEX OXIDE. Acta Metall Sin, 1991, 27(6): 158-159.

Download:  PDF(186KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The ultrafine alloy powders, CuRh, γ-Ni_(0.33)Fe_(0.66) and α-Fe_(0.66)Co_(0.33) of size less than 35 nm were prepared by reduction of complex metallic oxides under atmosphere of 15%H_2 and 85% Ar.
Key words:  ultrafine alloy powder      reduction      thermogravimetric analysjs      X-ray diffraction     
Received:  18 June 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I6/158

1 葛庭燧.材料科学与工程,1989;(1) :4
2 加藤哲男.日本金属学会会报,1989;28:977
3 Birringer R, et al. Trans Jpn Inst Met, 1986; 27(suppl.): 743
4 1959; 32: 1502
5 Hayashi Y, Sueyoshi T, Hirai S, Kishimoto M, Tashita K, Amemiya M. Eur Pat Appl, EP 56, 257, 1982
6 Wickham D G. Inorg Synth, 1967; 9: 152
7 Qian Yi-Tai, Kershaw R, Dwight K, Wold A. Mater Res Bull, 1983; 18: 543
8 Luo Huey-Lin, Duwez P. J Less-Common Met, 1964; 6: 24
[1] LI Shilei, LI Yang, WANG Youkang, WANG Shengjie, HE Lunhua, SUN Guang'ai, XIAO Tiqiao, WANG Yandong. Multiscale Residual Stress Evaluation of Engineering Materials/Components Based on Neutron and Synchrotron Radiation Technology[J]. 金属学报, 2023, 59(8): 1001-1014.
[2] WANG Fuqiang, LIU Wei, WANG Zhaowen. Effect of Local Cathode Current Increasing on Bath-Metal Two-Phase Flow Field in Aluminum Reduction Cells[J]. 金属学报, 2020, 56(7): 1047-1056.
[3] LI Yizhuang,HUANG Mingxin. A Method to Calculate the Dislocation Density of a TWIP Steel Based on Neutron Diffraction and Synchrotron X-Ray Diffraction[J]. 金属学报, 2020, 56(4): 487-493.
[4] XU Shuai, SUN Xinjun, LIANG Xiaokai, LIU Jun, YONG Qilong. Effect of Hot Rolling Deformation on Microstructure and Mechanical Properties of a High-Ti Wear-Resistant Steel[J]. 金属学报, 2020, 56(12): 1581-1591.
[5] LI Changji,ZOU Minjie,ZHANG Lei,WANG Yuanming,WANG Sucheng. High-Resolution X-Ray Diffraction Analysis of Epitaxial Films[J]. 金属学报, 2020, 56(1): 99-111.
[6] Yongli JIN,Hai YU,Jieyu ZHANG,Zengwu ZHAO. Effects of Magnetic Field on Reduction of CaOContaining Iron Oxides[J]. 金属学报, 2019, 55(3): 410-416.
[7] Weifeng HE, Xiang LI, Xiangfan NIE, Yinghong LI, Sihai LUO. Study on Stability of Residual Stress Induced by Laser Shock Processing in Titanium Alloy Thin-Components[J]. 金属学报, 2018, 54(3): 411-418.
[8] Yutuo ZHANG,Cong LI,Pei WANG,Dianzhong LI. IN SITU SYNCHROTRON X-RAY DIFFRACTION INVESTIGATION ON TENSILE PROPERTIES OF 9Ni STEEL[J]. 金属学报, 2016, 52(4): 403-409.
[9] Shenghua ZHANG,Pei WANG,Dianzhong LI,Yiyi LI. INVESTIGATION OF TRIP EFFECT IN ZG06Cr13Ni4Mo MARTENSITIC STAINLESS STEEL BY IN SITU SYNCHROTRON HIGH ENERGY X-RAY DIFFRACTION[J]. 金属学报, 2015, 51(11): 1306-1314.
[10] DAI Wenbin WANG Xinli YU Jingkun ZOU Zongshu. PRODUCTION OF MgAlON BY CARBOTHERMAL REDUCTION AND NITRIDATION[J]. 金属学报, 2011, 47(11): 1440-1444.
[11] LV Dongsheng; LI Weishan; TAN Chunlin; ZE Ronghua. PREPARATION AND ELECTROCHEMICAL BEHAVIORS OF Co-B ALLOY POWDERS[J]. 金属学报, 2010, 46(3): 346-351.
[12] LIN Qiyong ZHU Miaoyong. INFLUENCE OF CASTING SPEED ON SOFT REDUCTION GRADIENT IN CONTINUOUS CASTING BLOOM[J]. 金属学报, 2009, 45(2): 253-256.
[13] ;. Investigation on Preparation of Tb2Fe17 by Direct Electrochemical Reduction of Tb4O7-Fe2O3 Pellet in Molten Calcium Chloride[J]. 金属学报, 2008, 44(7): 859-862 .
[14] Zhao Ning. THE LIQUID STRUCTURE OF SN-CU LEAD-FREE SOLDERS[J]. 金属学报, 2008, 44(4): 467-472 .
[15] LIN Qi-Yong. Soft Reduction Gradient for Continuous Casting Slab with Different Steel Grade[J]. 金属学报, 2007, 43(12): 1297-1300 .
No Suggested Reading articles found!