TEM STUDY OF SECONDARY HARDENING OF MARTENSITE IN HIGH SPEED STEEL
QIU Jun; YUAN Yi; CHEN Jingrong(University of Science and Technology Beijing)
Cite this article:
QIU Jun; YUAN Yi; CHEN Jingrong(University of Science and Technology Beijing). TEM STUDY OF SECONDARY HARDENING OF MARTENSITE IN HIGH SPEED STEEL. Acta Metall Sin, 1992, 28(7): 19-24.
Abstract The precipitate phases of M42 matrix high speed steel, containing 4%Co, tempered in temperature range of 250 to 700℃ have been investigated. M_3C precipitate, mainly Fe_3C, occurs in the steel tempered at lower temperature, and lessens gradually over 400℃. Changing of diffracted streaks and fcc M_2C, mainly Mo_2C, are observed after tempered at 500 —560℃ and 580℃ respectively. When tempering temperature up to 700℃, all fcc M_2C transforms into hcp M_2C, and also VC, Cr_(23)C_6. The diffracted streaks are believed to be due to the segregation of alloying elements Mo and W together with C on {100}_α′,, and the change from mix-cluster to transition phase fcc M_2C, which results in secondary hardening of M42 matrix steel after tempering.
1 Kuo Kehsin. J Iron Steel Inst, 1953; 174: 223 Kuo Kehsin. J Iron Steel Inst, 1953; 173: 363 2 Fischmeister H F, Karagoez S, Andren H O. Acta Metall, 1988; 36: 817 3 陈景榕,朱煜铎.金属科学与工艺,1986;5(1) :1 4 郭可信.X射线学及电子显微术的进展.上海:上海科学技术出版社,1966:36 5 Edington J W. Practical Electron Microscopy in Materials Science. Part Ⅱ, 1971:70 6 Jack K H. Nitriding, Heat Treatment. London: The Metals Society, 1973 7 E1 Rakayby A M, Mills B. Mater Sci Technol, 1986; 2: 175 8 Raynor D, Whiteman J A, Honeycombe R W K. J Iron Steel Inst, 1966; 204: 1114