| FATIGUE PROPERTIES OF AN Al-Li ALLOY |
| AI Suhua;WANG Zhongguang;ZHANG Yun;HU Zhuangqi State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; Academia Sinica; Shenyang |
|
Cite this article:
AI Suhua;WANG Zhongguang;ZHANG Yun;HU Zhuangqi State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; Academia Sinica; Shenyang. FATIGUE PROPERTIES OF AN Al-Li ALLOY. Acta Metall Sin, 1993, 29(1): 33-38.
|
|
|
Abstract The room temperature fatigue life of smooth specimens for alloy 8090 hasbeen investigated in natural ageing and artificial ageing conditions. The high temperature fa-tigue properties were also studied at 100--200℃. A parallel study was also made on tradi-tional Al alloys LC4 (artificial ageing) and LY12(natural aging)for comparison. The results showed that the artificially aged state resulted in an increase in fatigue life incomparison with the naturally aged state. As compared with the traditional high strength al-loys LC4 and LY12 both the artificially aged and naturally aged states caused a significantenhancement in fatigue life. The fatigue life reduced markedly with increasing temperature forartificially aged alloy 8090. Though high temperarure fatigue life decreased a little for natural-ly aged alloys 8090 and LY12, there was increasing during 200℃ and 150℃, respectively. The observation of fracture surface demonstrated the fatigue cracks in alloy 8090 mainlyinitiated from the metallurgical defects on surfaces and subsurfaces. It also showed that thecharacter of laminated fracture was more obvious in alloy 8090 than in tranditional alumini-um.
|
|
Received: 18 January 1993
|
1 Sanders T H Jr., Starke E A Jr. Acta Metall, 1982; 30: 927 2 Gregson P J, Flower H M. Acta Metall, 1985; 33: 527 3 Flower H M, Gregson P J. Mater Sci Technol, 1987; 3: 81 4 Xu Y B, Wang Z G, Zhang Y, Zhao H H, Hu Z Q. Metall Trans. 1991; 22A: 723 5 刘玉林,张匀,赵洪恩,胡壮麒,师昌绪.金属学报,1991;27:A337 6 张匀.内部资料,1991G |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|