Please wait a minute...
Acta Metall Sin  1993, Vol. 29 Issue (3): 1-5    DOI:
Current Issue | Archive | Adv Search |
CCT-DIAGRAM OF Si-Mn-Mo ALLOY SYSTEM BAINITIC STEELS
LIU Xiao;ZHANG Mingxing;CHEN Daming;ZHOU Lubin;KANG Mokuang Northwestern Polytechnical University; Xi'an Faculty No.401; Northwestern Polytechnical University; Xi'an 710072
Cite this article: 

LIU Xiao;ZHANG Mingxing;CHEN Daming;ZHOU Lubin;KANG Mokuang Northwestern Polytechnical University; Xi'an Faculty No.401; Northwestern Polytechnical University; Xi'an 710072. CCT-DIAGRAM OF Si-Mn-Mo ALLOY SYSTEM BAINITIC STEELS. Acta Metall Sin, 1993, 29(3): 1-5.

Download:  PDF(1303KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  CCT-diagrams of Si-Mn-Mo system bainitic steel have been determined.With Mo 0.25%, the high-temperature transformation of the steel shifts large to the right,and the bainitic transformation becomes a "flat topped C-curve" at cooling rate in widerange. Si in the steel may cause a shift of the bainitic transformation region towards the right,and of the pro-eutectoid ferritic transformation region towards the left. Mn may delay thehigh temperature transformation more violently than the bainitic transformation.
Key words:  meta-bainite      bainitic steel      CCT-curve     
Received:  18 March 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I3/1

1 刘晓等,钢铁,待发表
2 康沫狂等,材料科学进展,1988. 2(3) :12
3 Kang M K, Chen D M, Yang D P, Hu G L. Metall Trans. 1992: 23A: 785
4 Cias W W, Doane D V. Metall Trans, 1973; 4A: 225
[1] LIU Man, HU Haijiang, TIAN Junyu, XU Guang. Effect of Ausforming on the Microstructures and Mechanical Properties of an Ultra-High Strength Bainitic Steel[J]. 金属学报, 2021, 57(6): 749-756.
[2] PENG Yun,SONG Liang,ZHAO Lin,MA Chengyong,ZHAO Haiyan,TIAN Zhiling. Research Status of Weldability of Advanced Steel[J]. 金属学报, 2020, 56(4): 601-618.
[3] Yaqiang TIAN,Geng TIAN,Xiaoping ZHENG,Liansheng CHEN,Yong XU,Shihong ZHANG. C and Mn Elements Characterization and Stability of Retained Austenite in Different Locations ofQuenching and Partitioning Bainite Steels[J]. 金属学报, 2019, 55(3): 332-340.
[4] LAN Liangyun QIU Chunlin ZHAO Dewen LI Canming GAO Xiuhua DU Linxiu. MICROSTRUCTURAL CHARACTERS AND TOUGHNESS OF DIFFERENT SUB–REGIONS IN THE WELDING HEAT AFFECTED ZONE OF LOW CARBON BAINITIC STEEL[J]. 金属学报, 2011, 47(8): 1046-1054.
[5] GAO Guhui ZHANG Han BAI Bingzhe. EFFECT OF TEMPERING TEMPERATURE ON LOW TEMPERATURE IMPACT TOUGHNESS OF A LOW CARBON Mn-SERIES BAINITIC STEEL[J]. 金属学报, 2011, 47(5): 513-519.
[6] CUI Lei YANG Shanwu WANG Shutao GAO Kewei HE Xinlai. EFFECT OF DAMNIFICATION IN RUST LAYER ON CORROSION BEHAVIORS OF LOWCARBON BAINITIC STEEL IN THE ENVIRONMENT CONTAINING Cl−[J]. 金属学报, 2009, 45(4): 442-449.
[7] Shu-Tao WANG; Kewei GAO. CORROSION BEHAVIOR AND VARIATION OF APPARENT MECHANICAL PROPERTY OF ONE NEWLY-DEVELOPED LOW CARBON BAINITIC STEEL IN ENVIRONMENT CONTAINING CHLORIDE ION[J]. 金属学报, 2008, 44(9): 1116-1124 .
[8] LUAN Daocheng; WEI Chengfu;YANG Ge (Department of Materials Science and Engineering; Sichuan Institute of Technology; Chengdu 611744). TWINS AND ITS FORMATION MECHANISM IN LOWER META-BAINITE[J]. 金属学报, 1998, 34(1): 24-30.
[9] LI Fengzhao;GU Yingni;JIANG Jiang;AO Qing;SUN Dongsheng (College of Materials Science and Engineering; Shandong University of Technology; Jinan 250061). MULTI-COMPONENT MICRO-ALLOYED AIR COOLING BAINITIC STEELS[J]. 金属学报, 1997, 33(5): 492-498.
[10] ZHANG Mingxing;KANG Mokuang Baotou Institute of Iron and Steel Technology; Noghwestern Polytechnical University; Xian. INFLUENCE OF Si ON MICROSTRUCTURE AND PROPERTIES OF LOW CARBON BAINITIC STEELS[J]. 金属学报, 1993, 29(1): 6-10.
[11] CHEN Daming;KANG Mokuang Northwestern Polytechnical University; Xi'an; TAN Ruobing Institute of Metal Research; Academia Sinica; Shenyang. FATIGUE PROPERTIES OF META-BAINITE IN STEEL 40CrMnSiMoVA[J]. 金属学报, 1991, 27(6): 64-69.
No Suggested Reading articles found!