Abstract CCT-diagrams of Si-Mn-Mo system bainitic steel have been determined.With Mo 0.25%, the high-temperature transformation of the steel shifts large to the right,and the bainitic transformation becomes a "flat topped C-curve" at cooling rate in widerange. Si in the steel may cause a shift of the bainitic transformation region towards the right,and of the pro-eutectoid ferritic transformation region towards the left. Mn may delay thehigh temperature transformation more violently than the bainitic transformation.
|
|
Received: 18 March 1993
|
1 刘晓等,钢铁,待发表 2 康沫狂等,材料科学进展,1988. 2(3) :12 3 Kang M K, Chen D M, Yang D P, Hu G L. Metall Trans. 1992: 23A: 785 4 Cias W W, Doane D V. Metall Trans, 1973; 4A: 225 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|