| EFFECT OF LASER SCANNING SPEED ON PHASE CONSTITUTION AND WEAR RESISTANCE OF LASERCLADDING STELLITE HARD FACING ALLOY |
| XU Yourong;ZHANG Henghua;CHEN Daming;XIE Fuchun;XU Mingyu;CHEN Lanying;SU Baorong;QIAN Hongbin Shanghai University of Science and Technology Shanghai Optics and Fine Mechinery Research Institute; Academia Sinica professor;Department of Materials Science and Engineering;Shanghai University of Science and Technology; Shanghai 201800 |
|
Cite this article:
XU Yourong;ZHANG Henghua;CHEN Daming;XIE Fuchun;XU Mingyu;CHEN Lanying;SU Baorong;QIAN Hongbin Shanghai University of Science and Technology Shanghai Optics and Fine Mechinery Research Institute; Academia Sinica professor;Department of Materials Science and Engineering;Shanghai University of Science and Technology; Shanghai 201800. EFFECT OF LASER SCANNING SPEED ON PHASE CONSTITUTION AND WEAR RESISTANCE OF LASERCLADDING STELLITE HARD FACING ALLOY. Acta Metall Sin, 1993, 29(3): 30-34.
|
|
|
Abstract Effect of laser scanning speed on phase constitution, microstructure,microhardness and wear resistance of laser-cladding stellite hard facing alloy by using of across-flow-stype CO_2 laser of power 1. 5 kW has been investigated. The laser-cladding layeron the alloy consists of matrix phase of over-saturation solid solution γ(Co, Cr) and complexhexagonal carbide M_7C_3. Under certain condition, with fast laser scanning speed, the oversaturation solubility of elements increases in γ(Co, Cr), and the precipitation of the complexcarbide M_7C_3 decreases, so that the microhardness increases and the wear resistance de-creases. But at slower laser scanning speed, more complex carbide M_7C_3 may precipitate, andthe wear resistance may be improved. Therefore, it is believed that the principal factor in im-provement over wear resistance is the precipitation of carbide M_7C_3, while overmicrohardness is the over-saturation solubility of elements in matrix phase (Co, Cr).
|
|
Received: 18 March 1993
|
1 Atamert S, Bhadeshia H K D H. Metall. Trans, 1989: 20A: 1037 2 Sizoaz S, Mazumder J. Metall Trans, 1989: 20A: 2267, 2489 3 Glordan L. Proceeding 3rd Int. Cong. on Heat Treatment of Materials, 1983; 9--22--9--26 4 Kesel T. H, Fiore N F. J Mater for Energy Syst, 1981; 3: 7 5 Gnanamuthu D S. Applications of Lasers in Materials Processing. Metals Park. Ohio: ASM, 1979: 177 6 姜晓霞,中国机械工程学会材料学会第一届论文集 1986;521W |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|