| RESPONSE OF (Ti_xV(1-x))(C_yN_(1-y)) PARTICLES IN HSLA STEEL TO WELD THERMAL CYCLES |
| GUI Chibin;CUI Kun Huazhong University of Science and Technology; Wuhandoctor;Department of 2nd Mechanical Engineering;Huazhong University of Science and Technollogy;Wuhan 430074 |
|
Cite this article:
GUI Chibin;CUI Kun Huazhong University of Science and Technology; Wuhandoctor;Department of 2nd Mechanical Engineering;Huazhong University of Science and Technollogy;Wuhan 430074. RESPONSE OF (Ti_xV(1-x))(C_yN_(1-y)) PARTICLES IN HSLA STEEL TO WELD THERMAL CYCLES. Acta Metall Sin, 1993, 29(8): 77-80.
|
|
|
Abstract (Ti_xV_(1-x))(C_yN(1-y)) particles in HSLA steel, subjected to weld thermal cycles, wasobserved to lag behind in dissolution, which reduces with the increase of peak temperature.And the coarsening rate of these particles is very slow.
|
|
Received: 18 August 1993
|
1 Ion J C, Easterling K E, Ashby M F. Acta Metall, 1984; 32: 1949 2 Ashby M F, Easterling K E. Acta Metall, 1982; 30: 1969 3 桂赤斌,崔昆,李志远.焊接学报,1990;11:136 4 McCutcheon D B, McGrath J T, Godden M J, Ruddle G E, Weatherly G, Houghton D C. ASTM STP 792, 1982: 227 5 Cuddy L J,Lally J S,Porter L F.高强度低合金钢工艺与应用国际会议论文集(中译本,第二分册),鞍山钢铁公司钢铁研究所,1986:326 6 Suzuki S, Weatherly G C, Houghton D C. Acta Metall, 1987; 35: 341 7 肖纪美著,合金热力学(下册),北京钢铁学院1982:94 8 Matsuta S, Okumura N, Trans. ISIJ, 1978; 18: 198 |