Please wait a minute...
Acta Metall Sin  1994, Vol. 30 Issue (22): 476-480    DOI:
Current Issue | Archive | Adv Search |
SELF-PROPAGATING COMBUSTION SYNTHESIS OF NiAl/TiB_2 COMPOSITE
WANG Weimin; FU Zhengyi;YUAN Runzhang(Wuhan University of Technology)
Cite this article: 

WANG Weimin; FU Zhengyi;YUAN Runzhang(Wuhan University of Technology). SELF-PROPAGATING COMBUSTION SYNTHESIS OF NiAl/TiB_2 COMPOSITE. Acta Metall Sin, 1994, 30(22): 476-480.

Download:  PDF(328KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Investigation was carried out on physico-chemical and microstructural changes during self-propagating combustion synthesis of the Ni-Al-Ti-B system. The principal factor influenced on the process was found to be the amount of TiB_2 doped. Microstructural observation revealed that the average size of TiB_2 particles, grown in situ, is dependent on the synthesising temperature. Meanwhile,some TiB_2 fibres occurred on the synthesised products,and their amount as well as growth morphology seemed to be affected by the growing space.
Key words:  NiAl/TiB_2 composite      self-propagating combustion synthesis      micro structure      TiB_2 fibre     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I22/476

1HoltJB,MunirZA.JMaterSci,1986;21:2512MigamotoY,NakamotoT.JMaterRes,1986;1:7
[1] HUA Mingjian Institute of Aeronoutical Materials;Beijing;Post Box NO.81;LI Chunzhi;WANG Hongjian Institute of Aeronautical Materials; Beijing. EFFECT OF MICROSTRUCTURES ON THE YIELD STRENGTH AND SCR OF 7075 ALUMINIUM ALLOY[J]. 金属学报, 1988, 24(1): 41-46.
No Suggested Reading articles found!